Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.352 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTl2SnSe3 + HgSe |
Band Gap0.889 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42m [121] |
HallI 4 2 |
Point Group42m |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tl3In2Se5 (mp-686102) | 0.3160 | 0.001 | 3 |
Tl3In7Se10 (mp-675519) | 0.3944 | 0.034 | 3 |
Tl2In3Se5 (mp-685385) | 0.3984 | 0.016 | 3 |
TlInSe2 (mp-22232) | 0.3996 | 0.000 | 3 |
KSnSe2 (mp-571016) | 0.3685 | 0.095 | 3 |
Tl2HgGeTe4 (mp-569246) | 0.1899 | 0.006 | 4 |
Tl2CdGeTe4 (mp-568890) | 0.1729 | 0.004 | 4 |
K2SnHgSe4 (mp-568968) | 0.0749 | 0.000 | 4 |
K2CdSnSe4 (mp-1079645) | 0.0918 | 0.000 | 4 |
Rb2SnHgTe4 (mp-1080691) | 0.1776 | 0.000 | 4 |
TlSe (mp-1836) | 0.3982 | 0.000 | 2 |
TlS (mp-322) | 0.4300 | 0.052 | 2 |
InTe (mp-20320) | 0.4942 | 0.011 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tl_d Sn_d Hg Se |
Final Energy/Atom-3.2269 eV |
Corrected Energy-25.8151 eV
-25.8151 eV = -25.8151 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)