Final Magnetic Moment3.843 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.916 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImmm [71] |
Hall-I 2 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb(ThSe3)2 (mp-9523) | 0.2111 | 0.000 | 3 |
K(ThSe3)2 (mp-9522) | 0.2210 | 0.000 | 3 |
BaCaI4 (mp-753709) | 0.7069 | 0.069 | 3 |
K(USe3)2 (mp-12414) | 0.1244 | 0.000 | 3 |
K(NpSe3)2 (mp-1095186) | 0.1608 | 0.000 | 3 |
U2Te2PO (mp-1095312) | 0.6532 | 0.003 | 4 |
U2Te5 (mp-573810) | 0.6302 | 0.041 | 2 |
UTe3 (mp-8357) | 0.6048 | 0.071 | 2 |
ThTe3 (mp-1025522) | 0.6497 | 0.000 | 2 |
CeSe2 (mp-1096430) | 0.6117 | 0.025 | 2 |
UTe3 (mp-568948) | 0.6129 | 0.071 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U Tl_d Se |
Final Energy/Atom-6.0183 eV |
Corrected Energy-54.1645 eV
-54.1645 eV = -54.1645 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)