material

LaGaO3

ID:

mp-1078871


Tags: Lanthanum gallate - HT Lanthanum gallate

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.092 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.039 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.00 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
La4Ga2O9 + La3Ga5O12
Band Gap
3.374 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3c [161]
Hall
R 3 2"c
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 51036 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NaOsO3 (mp-998624) 0.1286 0.015 3
CuAgF3 (mp-998422) 0.0483 0.013 3
BaTbO3 (mp-548824) 0.1653 0.093 3
LaGaO3 (mp-3336) 0.1689 0.038 3
CuAgF3 (mp-1099573) 0.0955 0.013 3
La2ZnFeO6 (mvc-13418) 0.1471 0.015 4
La10Mg(Ga3O10)3 (mp-695030) 0.1532 0.050 4
La2MgMnO6 (mvc-10946) 0.1639 0.033 4
La2MgGeO6 (mp-11585) 0.1380 0.016 4
La2MgMnO6 (mp-19406) 0.1650 0.033 4
In2Ag (mp-760385) 0.6643 0.096 2
Hf2Ge (mp-1072256) 0.6654 0.622 2
In2Cu (mp-1072518) 0.7417 0.139 2
CaLa9Ti5Cr5O30 (mp-694926) 0.1938 0.063 5
Ca2La8Ti5Cr5O30 (mp-743953) 0.1971 0.046 5
SrLa7TiGa7O24 (mp-720505) 0.2537 0.015 5
SrLaMnRuO6 (mp-39239) 0.2831 0.094 5
SrLaMnRuO6 (mp-690590) 0.2820 0.094 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Ga (purity>99.95%), La2O3 (purity>99.95%), Mg(NO3)2(purity>99%) and Sr(NO3)2 (purity>99.5%) were used as the starting materials. Powders of the Sr- and Mg-doped LaGaO3 powders with the composi [...]
One of the major requirements for the development and commercialization of low-cost SOFCs is the reduction in the operating temperature. One of the methods to reach this aim is the use of solid electr [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition LaGaO3.

Text computed by synthesisproject.org.

Calculation Summary

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: La Ga_d O
Final Energy/Atom
-7.2413 eV
Corrected Energy
-76.5348 eV
Uncorrected energy = -72.4128 eV Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV Corrected energy = -76.5348 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 51039
  • 73764
  • 51038
  • 73763
  • 51037
  • 51036
  • 73762
Submitted by
User remarks:
  • Lanthanum gallate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)