Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.861 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density12.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToDyGePt + GePt |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/nmm [129] |
HallP 4ab 2ab 1ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
U(CuSi)2 (mp-22374) | 0.2079 | 0.000 | 3 |
Lu(CuSi)2 (mp-5346) | 0.2134 | 0.000 | 3 |
Lu(CuSn)2 (mp-1078587) | 0.2044 | 0.108 | 3 |
La(AlZn)2 (mp-569713) | 0.2115 | 0.000 | 3 |
Np(CrSi)2 (mp-12085) | 0.2130 | 0.284 | 3 |
La3Cu4(P2O)2 (mp-6309) | 0.6150 | 0.000 | 4 |
KIn4 (mp-22481) | 0.2107 | 0.000 | 2 |
EuAl4 (mp-990191) | 0.2053 | 0.000 | 2 |
EuAl4 (mp-582799) | 0.2382 | 0.000 | 2 |
CaAl4 (mp-1749) | 0.2019 | 0.002 | 2 |
RbIn4 (mp-21477) | 0.2390 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Dy_3 Ge_d Pt |
Final Energy/Atom-6.0602 eV |
Corrected Energy-60.6016 eV
-60.6016 eV = -60.6016 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)