Final Magnetic Moment0.038 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.539 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.019 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.21 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLu2InNi2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mbm [127] |
Hall-P 4 2ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nd2MgCu2 (mp-16638) | 0.0290 | 0.000 | 3 |
Ce2MgCu2 (mp-22810) | 0.0454 | 0.001 | 3 |
Ho2InNi2 (mp-1078878) | 0.0860 | 0.016 | 3 |
Er2InNi2 (mp-1079954) | 0.0828 | 0.020 | 3 |
Dy2InNi2 (mp-1080118) | 0.0917 | 0.017 | 3 |
Zr3Ga2 (mp-30684) | 0.2685 | 0.000 | 2 |
Th3Ge2 (mp-314) | 0.3603 | 0.000 | 2 |
Ta3Ga2 (mp-16756) | 0.3622 | 0.000 | 2 |
Nb3Ga2 (mp-11393) | 0.3534 | 0.000 | 2 |
Hf3Si2 (mp-2105) | 0.4039 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 In_d Ni_pv |
Final Energy/Atom-5.2096 eV |
Corrected Energy-52.0961 eV
Uncorrected energy = -52.0961 eV
Corrected energy = -52.0961 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)