Final Magnetic Moment0.258 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.456 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density15.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mbm [127] |
Hall-P 4 2ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
U2SnRu2 (mp-20705) | 0.2074 | 0.000 | 3 |
U2Co2Sn (mp-22360) | 0.1612 | 0.033 | 3 |
U2Fe2Sn (mp-21357) | 0.1717 | 0.000 | 3 |
Cr2InPd2 (mp-1084761) | 0.2303 | 0.458 | 3 |
U2SnIr2 (mp-1095100) | 0.2062 | 0.000 | 3 |
Y3Au2 (mp-1080493) | 0.2783 | 0.032 | 2 |
Dy3Pd2 (mp-12543) | 0.6304 | 0.000 | 2 |
Ca3Hg2 (mp-11288) | 0.5656 | 0.000 | 2 |
Si2Mo3 (mp-1087230) | 0.5322 | 0.140 | 2 |
Gd3Pd2 (mp-22077) | 0.6044 | 0.014 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U In_d Ir |
Final Energy/Atom-9.0583 eV |
Corrected Energy-90.5830 eV
Uncorrected energy = -90.5830 eV
Corrected energy = -90.5830 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)