Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.686 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mbm [127] |
Hall-P 4 2ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Gd2InGe2 (mp-639160) | 0.0627 | 0.000 | 3 |
Er2CdGe2 (mp-1079052) | 0.0128 | 0.000 | 3 |
Y2CdGe2 (mp-1079785) | 0.0401 | 0.000 | 3 |
Dy2CdGe2 (mp-1079838) | 0.0328 | 0.000 | 3 |
Gd2MgGe2 (mp-19945) | 0.0871 | 0.000 | 3 |
U3Si2 (mp-21346) | 0.4443 | 0.151 | 2 |
Np3Si2 (mp-1079895) | 0.3709 | 0.438 | 2 |
Pu3Si2 (mp-1080146) | 0.2815 | 0.000 | 2 |
Ce3Si2 (mp-1079007) | 0.4296 | 0.001 | 2 |
Sr2Pb3 (mp-669913) | 0.3359 | 0.010 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tm_3 Cd Ge_d |
Final Energy/Atom-4.5040 eV |
Corrected Energy-45.0399 eV
Uncorrected energy = -45.0399 eV
Corrected energy = -45.0399 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)