Final Magnetic Moment6.077 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.997 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.212 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.34 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTeBr4 + Br + N2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K2MoCl6 (mp-27826) | 0.0160 | 0.000 | 3 |
K2TaCl6 (mp-31363) | 0.0055 | 0.010 | 3 |
K2WCl6 (mp-568914) | 0.0205 | 0.000 | 3 |
Pt(I3N)2 (mp-1078594) | 0.0107 | 1.239 | 3 |
Nb(Br3N)2 (mp-1079379) | 0.0101 | 1.149 | 3 |
LiMgH6Ir (mp-866640) | 0.2529 | 0.000 | 4 |
Rb19O3 (mp-779582) | 0.6121 | 0.043 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Te Br N |
Final Energy/Atom-2.2103 eV |
Corrected Energy-23.8186 eV
Uncorrected energy = -19.8926 eV
Composition-based energy adjustment (-0.534 eV/atom x 6.0 atoms) = -3.2040 eV
Composition-based energy adjustment (-0.361 eV/atom x 2.0 atoms) = -0.7220 eV
Corrected energy = -23.8186 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)