Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.762 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/nmm [129] |
HallP 4ab 2ab 1ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YCuAs2 (mp-10991) | 0.1000 | 0.000 | 3 |
ErCuAs2 (mp-10993) | 0.0568 | 0.000 | 3 |
DyCuAs2 (mp-10992) | 0.0918 | 0.000 | 3 |
TmCuAs2 (mp-10994) | 0.0416 | 0.000 | 3 |
HoCuAs2 (mp-21364) | 0.0854 | 0.000 | 3 |
ZrCuSiP (mp-20588) | 0.3024 | 0.000 | 4 |
TiCuGeAs (mp-1078472) | 0.3303 | 0.046 | 4 |
ZrCuGeAs (mp-1078698) | 0.2219 | 0.000 | 4 |
ZrCuSiAs (mp-9929) | 0.3761 | 0.000 | 4 |
HfCuGeAs (mp-1080723) | 0.2441 | 0.000 | 4 |
CaPd2 (mp-1063133) | 0.6667 | 0.297 | 2 |
ThFe2 (mp-1062988) | 0.5250 | 0.384 | 2 |
EuPd2 (mp-1063311) | 0.7088 | 0.313 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 Cu_pv As |
Final Energy/Atom-5.2469 eV |
Corrected Energy-41.9753 eV
-41.9753 eV = -41.9753 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)