Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.489 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr8Ni50Mo15W2 (mp-767372) | 0.5925 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.5856 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.5648 | 0.193 | 4 |
TiCd (mp-30500) | 0.2378 | 0.000 | 2 |
TiSi (mp-22558) | 0.2773 | 0.240 | 2 |
ZrIn3 (mp-1078602) | 0.0758 | 0.005 | 2 |
ZrAl3 (mp-395) | 0.2023 | 0.000 | 2 |
HfAl3 (mp-568718) | 0.2315 | 0.000 | 2 |
Hg (mp-569360) | 0.4418 | 0.001 | 1 |
Rb (mp-975519) | 0.4434 | 0.017 | 1 |
Eu (mp-1057315) | 0.4225 | 0.000 | 1 |
Ba (mp-1058581) | 0.3812 | 0.019 | 1 |
In (mp-1055994) | 0.4316 | 0.030 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zr_sv Ga_d |
Final Energy/Atom-4.8970 eV |
Corrected Energy-39.1760 eV
-39.1760 eV = -39.1760 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)