Final Magnetic Moment4.053 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.080 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnTe2 + Mn |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypePlane
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr10Sb3Te7 (mp-676935) | 0.4673 | 0.151 | 3 |
LiNi9S10 (mp-676685) | 0.5042 | 0.095 | 3 |
LiNi9S10 (mp-774863) | 0.4833 | 0.102 | 3 |
Ni2SbTe (mp-676310) | 0.4709 | 0.010 | 3 |
Co2SbTe (mp-675568) | 0.2966 | 0.043 | 3 |
SnIr (mp-20033) | 0.1213 | 0.000 | 2 |
NiAs (mp-590) | 0.1228 | 0.006 | 2 |
TeRh (mp-1628) | 0.1192 | 0.023 | 2 |
MnTe (mp-909046) | 0.1231 | 0.010 | 2 |
AuSe (mp-10678) | 0.1168 | 0.252 | 2 |
K (mp-1068966) | 0.7234 | 0.179 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mn_pv Te |
Final Energy/Atom-6.2326 eV |
Corrected Energy-49.8606 eV
-49.8606 eV = -49.8606 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)