Final Magnetic Moment0.014 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.075 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.528 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCeSe2 |
Band Gap1.028 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ag3AuS2 (mp-34460) | 0.5437 | 0.000 | 3 |
Si(CN2)2 (mp-30160) | 0.5290 | 0.028 | 3 |
Be(CN)2 (mp-35687) | 0.5220 | 0.226 | 3 |
AlPO4 (mp-545974) | 0.3363 | 0.011 | 3 |
Mg2ZnN2 (mp-1029265) | 0.4890 | 1.954 | 3 |
LiB(CN)4 (mp-13590) | 0.6255 | 0.336 | 4 |
CuB(CN)4 (mp-13589) | 0.5771 | 0.351 | 4 |
CuCSN (mp-672285) | 0.6931 | 0.157 | 4 |
CuCSN (mp-559044) | 0.6901 | 0.157 | 4 |
LiCo(CO)4 (mp-18939) | 0.5764 | 0.407 | 4 |
SiO2 (mp-7087) | 0.0463 | 0.012 | 2 |
SiO2 (mp-8352) | 0.0014 | 0.012 | 2 |
CrN2 (mp-1014373) | 0.0008 | 0.342 | 2 |
Hg2N (mp-1077346) | 0.0004 | 0.716 | 2 |
CrN2 (mp-1015780) | 0.2535 | 0.340 | 2 |
C (mp-1095534) | 0.6937 | 1.121 | 1 |
C (mp-1095633) | 0.7411 | 0.997 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce Se |
Final Energy/Atom-5.3837 eV |
Corrected Energy-34.1901 eV
Uncorrected energy = -32.3021 eV
Composition-based energy adjustment (-0.472 eV/atom x 4.0 atoms) = -1.8880 eV
Corrected energy = -34.1901 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)