Final Magnetic Moment1.706 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.999 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.127 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.78 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSb2Se3 + Ce10Se19 + Sb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2N2O (mp-780050) | 0.6234 | 0.087 | 3 |
La4Mn4O11 (mp-763616) | 0.6691 | 0.122 | 3 |
Zn(CoO2)2 (mvc-12655) | 0.6599 | 0.189 | 3 |
Li8Mn5O10 (mp-764701) | 0.6541 | 0.038 | 3 |
Li4Bi3O8 (mp-769008) | 0.6327 | 0.065 | 3 |
Li7Mn(OF)3 (mp-767191) | 0.7166 | 0.273 | 4 |
Li4Co3OF8 (mp-763942) | 0.6279 | 0.072 | 4 |
Li7V(O2F)2 (mp-765831) | 0.6884 | 0.103 | 4 |
KCu(BiS2)2 (mp-558063) | 0.7328 | 0.000 | 4 |
Li4Fe3OF8 (mp-764594) | 0.6144 | 0.078 | 4 |
Y2O3 (mp-775907) | 0.7071 | 0.053 | 2 |
Ho2S3 (mp-878) | 0.5802 | 0.000 | 2 |
V2O3 (mp-776630) | 0.6504 | 0.086 | 2 |
Y2S3 (mp-541289) | 0.5769 | 0.000 | 2 |
Er2S3 (mp-2234) | 0.5819 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce Sb Se |
Final Energy/Atom-5.1768 eV |
Corrected Energy-186.3661 eV
-186.3661 eV = -186.3661 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)