Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.087 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.516 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.49 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCeSe2 |
Band Gap1.021 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-5724) | 0.4436 | 0.003 | 3 |
AlPO4 (mp-557362) | 0.4717 | 0.010 | 3 |
AlPO4 (mp-558056) | 0.4327 | 0.011 | 3 |
AlPO4 (mp-1019510) | 0.4418 | 0.010 | 3 |
CoPO4 (mp-694829) | 0.4773 | 0.196 | 3 |
RbAlSiO4 (mp-6434) | 0.6783 | 0.000 | 4 |
CsAlSiO4 (mp-561457) | 0.5425 | 0.000 | 4 |
CsFeSiO4 (mp-644325) | 0.6469 | 0.000 | 4 |
KBePO4 (mp-7324) | 0.7087 | 0.000 | 4 |
CsBePO4 (mp-15395) | 0.5625 | 0.000 | 4 |
SiO2 (mp-557930) | 0.2422 | 0.032 | 2 |
SiO2 (mp-562490) | 0.2150 | 0.010 | 2 |
SiO2 (mp-555740) | 0.2140 | 0.032 | 2 |
CeSe2 (mp-1080256) | 0.2179 | 0.516 | 2 |
CeSe2 (mp-1080261) | 0.1781 | 0.515 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce Se |
Final Energy/Atom-5.3954 eV |
Corrected Energy-68.5212 eV
Uncorrected energy = -64.7452 eV
Composition-based energy adjustment (-0.472 eV/atom x 8.0 atoms) = -3.7760 eV
Corrected energy = -68.5212 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)