Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.067 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.535 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.27 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCeSe2 |
Band Gap0.663 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4122 [98] |
HallI 4bw 2bw |
Point Group422 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VBO4 (mp-771386) | 0.6517 | 0.068 | 3 |
AlPO4 (mp-560815) | 0.7297 | 0.030 | 3 |
LiCu(PO3)2 (mp-25975) | 0.7409 | 0.047 | 4 |
CsSi3HO7 (mp-758180) | 0.7483 | 0.002 | 4 |
KBePO4 (mp-7324) | 0.7364 | 0.000 | 4 |
Na2Be(SiO3)2 (mp-560438) | 0.7462 | 0.050 | 4 |
Si2O5 (mp-862998) | 0.4675 | 0.593 | 2 |
SiO2 (mp-545719) | 0.4937 | 0.150 | 2 |
SiO2 (mp-559860) | 0.4841 | 0.160 | 2 |
SiO2 (mp-556588) | 0.5172 | 0.303 | 2 |
SiO2 (mp-560954) | 0.4501 | 0.169 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce Se |
Final Energy/Atom-5.3758 eV |
Corrected Energy-129.0190 eV
-129.0190 eV = -129.0190 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)