Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.078 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.525 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCeSe2 |
Band Gap0.963 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mcm [140] |
Hall-I 4 2c |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BePO4 (mp-760410) | 0.2793 | 0.063 | 3 |
AlPO4 (mp-707977) | 0.3263 | 0.010 | 3 |
AlPO4 (mp-541338) | 0.3334 | 0.012 | 3 |
AlPO4 (mp-561027) | 0.3622 | 0.012 | 3 |
AlPO4 (mp-559145) | 0.3478 | 0.013 | 3 |
CsBeAsO4 (mp-9113) | 0.7061 | 0.000 | 4 |
Cs2MgSi5O12 (mp-1019610) | 0.6935 | 0.000 | 4 |
CsBePO4 (mp-15395) | 0.6905 | 0.000 | 4 |
SiO2 (mp-18280) | 0.1344 | 0.008 | 2 |
SiO2 (mp-554258) | 0.0753 | 0.009 | 2 |
SiO2 (mp-555556) | 0.1351 | 0.009 | 2 |
CeSe2 (mp-1080363) | 0.1414 | 0.524 | 2 |
SiO2 (mp-16964) | 0.1360 | 0.008 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce Se |
Final Energy/Atom-5.3865 eV |
Corrected Energy-258.5514 eV
-258.5514 eV = -258.5514 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)