material

VIr3

ID:

mp-1082

DOI:

10.17188/1187380


Tags: Iridium vanadium (3/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.496 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.022 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
18.41 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
VIr3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 104594 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ge (mp-32) <1 0 0> <1 0 0> 0.003 132.7
Ge (mp-32) <1 1 0> <1 1 0> 0.003 187.6
Cu (mp-30) <1 0 0> <1 0 0> 0.006 117.9
Cu (mp-30) <1 1 0> <1 1 0> 0.006 166.8
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.010 76.6
GaAs (mp-2534) <1 0 0> <1 0 0> 0.015 132.7
GaAs (mp-2534) <1 1 0> <1 1 0> 0.017 187.6
AlN (mp-661) <0 0 1> <1 1 1> 0.028 25.5
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.032 166.8
TeO2 (mp-2125) <1 0 1> <1 0 0> 0.044 309.6
InSb (mp-20012) <1 1 0> <1 1 0> 0.044 62.5
InSb (mp-20012) <1 1 1> <1 1 1> 0.045 76.6
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.048 62.5
LiF (mp-1138) <1 0 0> <1 0 0> 0.050 132.7
LiF (mp-1138) <1 1 0> <1 1 0> 0.053 187.6
BN (mp-984) <1 1 0> <1 1 0> 0.055 166.8
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.055 132.7
MgO (mp-1265) <1 1 0> <1 1 0> 0.056 229.3
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.059 187.6
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.069 132.7
CdTe (mp-406) <1 1 0> <1 1 0> 0.069 62.5
CdTe (mp-406) <1 1 1> <1 1 1> 0.071 76.6
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.073 187.6
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.081 25.5
ZrO2 (mp-2858) <1 1 0> <1 0 0> 0.084 280.1
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.122 221.1
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.124 83.4
C (mp-48) <1 0 1> <1 0 0> 0.125 221.1
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.169 294.8
DyScO3 (mp-31120) <1 1 1> <1 0 0> 0.179 280.1
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.195 62.5
SiC (mp-7631) <1 0 1> <1 0 0> 0.234 235.8
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.237 73.7
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.245 221.1
TbScO3 (mp-31119) <0 1 0> <1 1 1> 0.247 306.4
Al2O3 (mp-1143) <1 0 0> <1 0 0> 0.252 250.6
LaAlO3 (mp-2920) <1 1 1> <1 1 1> 0.261 127.7
CdWO4 (mp-19387) <1 0 0> <1 0 0> 0.262 309.6
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.273 125.1
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.322 29.5
PbSe (mp-2201) <1 1 0> <1 1 0> 0.325 166.8
ZrO2 (mp-2858) <0 1 1> <1 0 0> 0.338 309.6
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.343 41.7
Si (mp-149) <1 0 0> <1 0 0> 0.344 29.5
ZnO (mp-2133) <1 0 1> <1 0 0> 0.346 221.1
Te2W (mp-22693) <1 0 0> <1 1 0> 0.350 291.8
TbScO3 (mp-31119) <1 1 1> <1 0 0> 0.350 280.1
C (mp-66) <1 1 1> <1 1 0> 0.354 333.5
Si (mp-149) <1 1 0> <1 1 0> 0.367 41.7
CaCO3 (mp-3953) <0 0 1> <1 1 0> 0.368 333.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
534 213 213 0 0 0
213 534 213 0 0 0
213 213 534 0 0 0
0 0 0 261 0 0
0 0 0 0 261 0
0 0 0 0 0 261
Compliance Tensor Sij (10-12Pa-1)
2.4 -0.7 -0.7 0 0 0
-0.7 2.4 -0.7 0 0 0
-0.7 -0.7 2.4 0 0 0
0 0 0 3.8 0 0
0 0 0 0 3.8 0
0 0 0 0 0 3.8
Shear Modulus GV
221 GPa
Bulk Modulus KV
320 GPa
Shear Modulus GR
209 GPa
Bulk Modulus KR
320 GPa
Shear Modulus GVRH
215 GPa
Bulk Modulus KVRH
320 GPa
Elastic Anisotropy
0.29
Poisson's Ratio
0.23

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.1125 0.005 3
CrCoPt2 (mp-570863) 0.0492 0.000 3
LiCa6Ge (mp-12609) 0.0000 0.180 3
GaFeNi2 (mp-1065359) 0.0412 0.066 3
GaCo2Ni (mp-1018060) 0.0157 0.075 3
Cr8Ni50Mo15W2 (mp-767372) 0.2155 0.028 4
CrFeCoNi (mp-1012640) 0.3608 0.118 4
CrFeCoNi (mp-1096923) 0.4019 0.193 4
Rb3Hg (mp-974951) 0.0000 0.077 2
PmSn3 (mp-862960) 0.0000 0.000 2
HfPd3 (mp-1007656) 0.0000 0.014 2
NdSn3 (mp-1977) 0.0000 0.000 2
Ca3Mg (mp-1094857) 0.0000 0.025 2
Sr (mp-76) 0.0000 0.006 1
N2 (mp-1056857) 0.0000 0.000 1
Ni (mp-1056486) 0.0000 0.000 1
Cd (mp-1096861) 0.0000 0.001 1
Pd (mp-1056438) 0.0000 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: V_pv Ir
Final Energy/Atom
-9.3959 eV
Corrected Energy
-37.5836 eV
Uncorrected energy = -37.5836 eV Corrected energy = -37.5836 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 104594
  • 641154
Submitted by
User remarks:
  • Iridium vanadium (3/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)