Final Magnetic Moment0.068 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.064 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density19.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 226.2 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 226.2 |
Au (mp-81) | <1 0 0> | <1 0 0> | 226.2 |
Ni (mp-23) | <1 1 1> | <1 1 0> | 319.9 |
Cu (mp-30) | <1 1 1> | <1 1 1> | 293.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 282.8 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 282.8 |
YAlO3 (mp-3792) | <1 0 0> | <1 1 0> | 80.0 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 160.0 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 113.1 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 282.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 226.2 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 160.0 |
C (mp-48) | <0 0 1> | <1 0 0> | 226.2 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 240.0 |
TiO2 (mp-390) | <1 0 1> | <1 1 0> | 80.0 |
ZrO2 (mp-2858) | <1 1 -1> | <1 0 0> | 226.2 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 98.0 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 319.9 |
ZnO (mp-2133) | <1 1 0> | <1 1 0> | 240.0 |
WSe2 (mp-1821) | <0 0 1> | <1 0 0> | 339.4 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 339.4 |
Cu (mp-30) | <1 0 0> | <1 1 1> | 195.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 169.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 169.7 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 293.9 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 319.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 282.8 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 1> | 293.9 |
MgF2 (mp-1249) | <1 1 1> | <1 1 0> | 240.0 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 169.7 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 282.8 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 56.6 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 282.8 |
Fe2O3 (mp-24972) | <0 0 1> | <1 1 1> | 293.9 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 282.8 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 282.8 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 0> | 282.8 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 113.1 |
TiO2 (mp-2657) | <1 1 1> | <1 1 1> | 293.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 282.8 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 282.8 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 1> | 293.9 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 160.0 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 319.9 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 226.2 |
GaTe (mp-542812) | <1 0 0> | <1 0 0> | 226.2 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 160.0 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 282.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 160.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
233 | 241 | 241 | 0 | 0 | 0 |
241 | 233 | 241 | 0 | 0 | 0 |
241 | 241 | 233 | 0 | 0 | 0 |
0 | 0 | 0 | 21 | 0 | 0 |
0 | 0 | 0 | 0 | 21 | 0 |
0 | 0 | 0 | 0 | 0 | 21 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-85.5 | 43.4 | 43.4 | 0 | 0 | 0 |
43.4 | -85.5 | 43.4 | 0 | 0 | 0 |
43.4 | 43.4 | -85.5 | 0 | 0 | 0 |
0 | 0 | 0 | 46.6 | 0 | 0 |
0 | 0 | 0 | 0 | 46.6 | 0 |
0 | 0 | 0 | 0 | 0 | 46.6 |
Shear Modulus GV11 GPa |
Bulk Modulus KV238 GPa |
Shear Modulus GR-13 GPa |
Bulk Modulus KR238 GPa |
Shear Modulus GVRH-1 GPa |
Bulk Modulus KVRH238 GPa |
Elastic Anisotropy-9.25 |
Poisson's Ratio0.50 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbNi4Au (mp-1024977) | 0.0000 | 0.040 | 3 |
TmInCu4 (mp-1024957) | 0.0028 | 0.000 | 3 |
GdNi4Au (mp-1077131) | 0.0027 | 0.855 | 3 |
YbCu4Au (mp-1077165) | 0.0028 | 0.000 | 3 |
GdInCu4 (mp-1077293) | 0.0009 | 0.000 | 3 |
NdFe2 (mp-1207) | 0.0000 | 0.080 | 2 |
LuAl2 (mp-1234) | 0.0000 | 0.000 | 2 |
YMn2 (mp-558) | 0.0000 | 0.162 | 2 |
PbAu2 (mp-19871) | 0.0000 | 0.000 | 2 |
SmRu2 (mp-1720) | 0.0000 | 0.021 | 2 |
Co (mp-1072089) | 0.0000 | 0.199 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U Os_pv |
Final Energy/Atom-11.3128 eV |
Corrected Energy-67.8768 eV
-67.8768 eV = -67.8768 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)