material

Ca(Al2Cu)4

ID:

mp-10877

DOI:

10.17188/1187419


Tags: Aluminium calcium copper (8/1/4)

Material Details

Final Magnetic Moment
0.003 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.267 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.21 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 57539 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Mg (mp-153) <0 0 1> <1 0 0> 0.001 272.3
Cu (mp-30) <1 1 1> <1 0 0> 0.002 45.4
Au (mp-81) <1 0 0> <0 0 1> 0.006 157.1
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.007 272.3
WS2 (mp-224) <0 0 1> <1 0 0> 0.007 272.3
Au (mp-81) <1 1 1> <1 0 0> 0.009 90.8
Y3Fe5O12 (mp-19648) <1 0 0> <0 0 1> 0.010 157.1
BaF2 (mp-1029) <1 1 1> <1 0 0> 0.010 136.2
Te2Mo (mp-602) <1 0 0> <1 0 0> 0.012 272.3
CaF2 (mp-2741) <1 1 1> <1 0 0> 0.013 317.7
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.015 78.6
C (mp-48) <1 0 1> <1 1 0> 0.019 321.0
C (mp-48) <0 0 1> <1 0 0> 0.024 136.2
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.025 272.3
Fe2O3 (mp-24972) <0 0 1> <1 0 0> 0.028 45.4
Bi2Te3 (mp-34202) <0 0 1> <1 0 0> 0.029 136.2
GaP (mp-2490) <1 1 1> <1 0 0> 0.038 317.7
Ag (mp-124) <1 0 0> <0 0 1> 0.039 157.1
Ga2O3 (mp-886) <1 0 -1> <1 1 0> 0.040 192.6
Ag (mp-124) <1 1 1> <1 0 0> 0.047 90.8
GaN (mp-804) <1 0 1> <1 1 0> 0.049 192.6
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.050 314.2
CdS (mp-672) <1 0 0> <1 1 0> 0.052 256.8
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.053 314.2
BaTiO3 (mp-5986) <1 1 1> <1 1 1> 0.055 202.9
Mg (mp-153) <1 0 1> <1 0 0> 0.074 317.7
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.075 317.7
BN (mp-984) <1 0 1> <1 1 1> 0.086 101.4
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.091 314.2
PbSe (mp-2201) <1 0 0> <0 0 1> 0.092 78.6
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.097 317.7
SiC (mp-11714) <1 1 0> <1 0 1> 0.100 272.2
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.101 157.1
PbSe (mp-2201) <1 1 1> <1 0 0> 0.102 136.2
DyScO3 (mp-31120) <0 1 1> <1 1 0> 0.104 321.0
AlN (mp-661) <0 0 1> <1 0 0> 0.104 317.7
Cu (mp-30) <1 0 0> <1 0 0> 0.105 317.7
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.114 136.2
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.115 136.2
GaSb (mp-1156) <1 0 0> <0 0 1> 0.131 78.6
LiGaO2 (mp-5854) <0 1 1> <1 1 0> 0.134 128.4
ZnTe (mp-2176) <1 1 0> <1 0 1> 0.136 272.2
Te2W (mp-22693) <0 1 0> <1 0 0> 0.139 272.3
GaSb (mp-1156) <1 1 1> <1 0 0> 0.142 136.2
InAs (mp-20305) <1 1 0> <1 0 1> 0.143 272.2
InP (mp-20351) <1 0 0> <0 0 1> 0.150 314.2
Te2W (mp-22693) <1 0 0> <1 1 0> 0.155 192.6
C (mp-66) <1 1 0> <1 0 0> 0.158 90.8
TbScO3 (mp-31119) <0 1 1> <1 1 0> 0.163 321.0
CsI (mp-614603) <1 0 0> <0 0 1> 0.164 314.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
186 46 46 0 0 0
46 174 58 0 0 0
46 58 174 0 0 0
0 0 0 66 0 0
0 0 0 0 60 0
0 0 0 0 0 60
Compliance Tensor Sij (10-12Pa-1)
6 -1.2 -1.2 0 0 0
-1.2 6.7 -1.9 0 0 0
-1.2 -1.9 6.7 0 0 0
0 0 0 15.1 0 0
0 0 0 0 16.6 0
0 0 0 0 0 16.6
Shear Modulus GV
63 GPa
Bulk Modulus KV
93 GPa
Shear Modulus GR
63 GPa
Bulk Modulus KR
93 GPa
Shear Modulus GVRH
63 GPa
Bulk Modulus KVRH
93 GPa
Elastic Anisotropy
0.02
Poisson's Ratio
0.22

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Y(Al2Cu)4 (mp-11029) 0.0857 0.000 3
Dy(Al2Cu)4 (mp-984726) 0.0855 0.000 3
Tm(Al2Cu)4 (mp-865864) 0.0874 0.000 3
Sm(Al2Cu)4 (mp-16498) 0.0920 0.000 3
Ce(Al2Cu)4 (mp-20003) 0.0306 0.000 3
Be12V (mp-571438) 0.2074 0.000 2
TaBe12 (mp-567842) 0.1995 0.000 2
Be12Pt (mp-571622) 0.1149 0.119 2
Be12Nb (mp-568912) 0.1759 0.000 2
Be12Pd (mp-12666) 0.1294 0.079 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Al Cu_pv
Final Energy/Atom
-3.9871 eV
Corrected Energy
-51.8320 eV
-51.8320 eV = -51.8320 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 57539
Submitted by
User remarks:
  • Aluminium calcium copper (8/1/4)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)