material

AlVNi2

ID:

mp-10899

DOI:

10.17188/1187440


Tags: Aluminium nickel vanadium (1/2/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.388 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.046 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.67 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
V3Ni2 + VNi2 + AlNi
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 58071 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-8062) <1 1 1> <1 1 1> 0.000 232.5
SiC (mp-7631) <0 0 1> <1 1 1> 0.001 58.1
SiC (mp-11714) <0 0 1> <1 1 1> 0.002 58.1
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.003 268.5
Si (mp-149) <1 0 0> <1 0 0> 0.005 268.5
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.006 167.8
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.011 94.9
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.020 67.1
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.020 134.2
MoSe2 (mp-1634) <1 1 0> <1 0 0> 0.020 268.5
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.022 94.9
LiF (mp-1138) <1 0 0> <1 0 0> 0.028 33.6
LiF (mp-1138) <1 1 0> <1 1 0> 0.031 47.5
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.031 167.8
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.033 174.4
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.045 167.8
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.049 142.4
GaSe (mp-1943) <0 0 1> <1 1 0> 0.055 189.8
TeO2 (mp-2125) <1 0 1> <1 0 0> 0.061 234.9
AlN (mp-661) <0 0 1> <1 1 0> 0.061 237.3
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.062 94.9
TiO2 (mp-390) <1 0 0> <1 0 0> 0.065 335.6
C (mp-66) <1 0 0> <1 0 0> 0.071 167.8
BN (mp-984) <1 1 1> <1 1 0> 0.076 237.3
Ge (mp-32) <1 0 0> <1 0 0> 0.076 33.6
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.080 268.5
MgO (mp-1265) <1 1 0> <1 1 0> 0.082 284.8
Ge (mp-32) <1 1 0> <1 1 0> 0.085 47.5
Ge (mp-32) <1 1 1> <1 1 1> 0.088 58.1
InAs (mp-20305) <1 0 0> <1 0 0> 0.103 302.0
ZnO (mp-2133) <0 0 1> <1 0 0> 0.104 167.8
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.106 94.9
KTaO3 (mp-3614) <1 1 1> <1 0 0> 0.115 167.8
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.119 302.0
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.123 302.0
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.127 142.4
Ga2O3 (mp-886) <0 1 0> <1 1 0> 0.132 142.4
BN (mp-984) <0 0 1> <1 1 0> 0.141 189.8
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.142 268.5
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.152 234.9
Mg (mp-153) <1 1 1> <1 0 0> 0.152 268.5
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.152 302.0
C (mp-48) <0 0 1> <1 0 0> 0.153 335.6
GaAs (mp-2534) <1 0 0> <1 0 0> 0.154 33.6
Al (mp-134) <1 1 1> <1 0 0> 0.165 167.8
GaAs (mp-2534) <1 1 0> <1 1 0> 0.170 47.5
WS2 (mp-224) <1 1 0> <1 1 1> 0.172 232.5
GaAs (mp-2534) <1 1 1> <1 1 1> 0.176 58.1
C (mp-66) <1 1 0> <1 1 0> 0.184 142.4
GaTe (mp-542812) <1 0 -1> <1 0 0> 0.185 302.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
196 168 168 0 0 0
168 196 168 0 0 0
168 168 196 0 0 0
0 0 0 111 0 0
0 0 0 0 111 0
0 0 0 0 0 111
Compliance Tensor Sij (10-12Pa-1)
24.4 -11.3 -11.3 0 0 0
-11.3 24.4 -11.3 0 0 0
-11.3 -11.3 24.4 0 0 0
0 0 0 9 0 0
0 0 0 0 9 0
0 0 0 0 0 9
Shear Modulus GV
72 GPa
Bulk Modulus KV
177 GPa
Shear Modulus GR
29 GPa
Bulk Modulus KR
177 GPa
Shear Modulus GVRH
51 GPa
Bulk Modulus KVRH
177 GPa
Elastic Anisotropy
7.26
Poisson's Ratio
0.37

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Mn2GaCo (mp-20160) 0.0000 0.147 3
TaGaNi2 (mp-21175) 0.0000 0.007 3
Li2GaPd (mp-3201) 0.0000 0.000 3
YInAu2 (mp-22493) 0.0000 0.000 3
DyInCu2 (mp-22680) 0.0000 0.020 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSnAu (mp-7554) 0.0000 0.088 4
VFeCoGe (mp-1063914) 0.0000 0.000 4
LiMgSbPd (mp-10179) 0.0000 0.096 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
SmMg3 (mp-30779) 0.0000 0.065 2
Ni3Sb (mp-10260) 0.0000 0.044 2
LiZn (mp-1934) 0.0000 0.000 2
LaF3 (mp-13181) 0.0000 0.181 2
CeCd3 (mp-2863) 0.0000 0.000 2
Pr (mp-63) 0.0000 0.136 1
Se (mp-119) 0.0000 0.602 1
He (mp-23158) 0.0000 0.000 1
Mo (mp-129) 0.0000 0.000 1
Tb (mp-11446) 0.0000 0.148 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Al V_pv Ni_pv
Final Energy/Atom
-6.4846 eV
Corrected Energy
-25.9383 eV
-25.9383 eV = -25.9383 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 58071
Submitted by
User remarks:
  • Aluminium nickel vanadium (1/2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)