material

Al3Pd2

ID:

mp-10901

DOI:

10.17188/1187444


Tags: Aluminium palladium (3/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.773 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.00 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 58117 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiNbO3 (mp-3731) <1 0 0> <1 0 0> 0.000 221.5
LiNbO3 (mp-3731) <1 0 1> <1 0 0> 0.000 155.0
PbS (mp-21276) <1 1 1> <0 0 1> 0.002 62.3
KTaO3 (mp-3614) <1 0 0> <1 0 1> 0.004 81.2
YAlO3 (mp-3792) <0 1 1> <1 1 0> 0.005 191.8
PbS (mp-21276) <1 0 0> <1 0 1> 0.006 108.3
TiO2 (mp-390) <0 0 1> <1 0 1> 0.011 216.6
MgO (mp-1265) <1 1 0> <1 1 0> 0.012 76.7
MgO (mp-1265) <1 0 0> <1 0 1> 0.014 54.2
Al (mp-134) <1 0 0> <1 0 1> 0.016 81.2
PbS (mp-21276) <1 1 0> <1 1 0> 0.020 153.4
PbSe (mp-2201) <1 1 1> <0 0 1> 0.021 202.5
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.028 66.4
KCl (mp-23193) <1 1 0> <1 1 0> 0.029 115.1
GaN (mp-804) <0 0 1> <0 0 1> 0.029 62.3
Cu (mp-30) <1 1 1> <0 0 1> 0.032 202.5
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.035 311.6
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.036 110.7
KCl (mp-23193) <1 0 0> <1 0 1> 0.041 81.2
Mg (mp-153) <1 0 0> <1 0 0> 0.041 66.4
GaSb (mp-1156) <1 1 1> <0 0 1> 0.045 202.5
GaN (mp-804) <1 0 1> <1 0 0> 0.047 132.9
CdTe (mp-406) <1 1 0> <1 0 0> 0.053 310.0
C (mp-48) <1 1 0> <1 0 0> 0.054 66.4
Fe3O4 (mp-19306) <1 0 0> <1 0 1> 0.058 216.6
InSb (mp-20012) <1 1 0> <1 0 0> 0.058 310.0
BaTiO3 (mp-5986) <1 1 0> <1 0 1> 0.061 216.6
TePb (mp-19717) <1 1 1> <0 0 1> 0.062 296.0
WS2 (mp-224) <0 0 1> <0 0 1> 0.070 62.3
Ga2O3 (mp-886) <1 1 0> <0 0 1> 0.070 296.0
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.071 62.3
CdSe (mp-2691) <1 1 1> <0 0 1> 0.071 202.5
NdGaO3 (mp-3196) <0 0 1> <1 1 1> 0.086 124.2
LiF (mp-1138) <1 1 0> <1 1 1> 0.098 165.6
YAlO3 (mp-3792) <1 0 1> <1 0 1> 0.100 243.7
MoSe2 (mp-1634) <1 0 0> <1 1 1> 0.112 207.0
Te2W (mp-22693) <1 0 1> <1 0 0> 0.115 199.3
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.121 109.1
GdScO3 (mp-5690) <1 1 0> <1 0 1> 0.121 324.9
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.122 202.5
LiAlO2 (mp-3427) <1 1 0> <1 0 1> 0.129 189.5
InP (mp-20351) <1 1 1> <0 0 1> 0.143 62.3
Mg (mp-153) <0 0 1> <0 0 1> 0.146 62.3
AlN (mp-661) <1 0 1> <1 1 1> 0.148 124.2
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.150 177.2
BaTiO3 (mp-5986) <0 0 1> <1 0 1> 0.159 81.2
LaF3 (mp-905) <1 1 0> <0 0 1> 0.159 93.5
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.165 311.6
ZnSe (mp-1190) <1 0 0> <1 0 1> 0.171 162.5
C (mp-48) <0 0 1> <0 0 1> 0.171 15.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
207 87 81 -7 0 0
87 207 81 7 0 0
81 81 247 0 0 0
-7 7 0 61 0 0
0 0 0 0 61 -7
0 0 0 0 -7 60
Compliance Tensor Sij (10-12Pa-1)
6.3 -2.2 -1.4 1 0 0
-2.2 6.3 -1.4 -1 0 0
-1.4 -1.4 5 0 0 0
1 -1 0 16.6 0 0
0 0 0 0 16.6 1.9
0 0 0 0 1.9 17
Shear Modulus GV
64 GPa
Bulk Modulus KV
129 GPa
Shear Modulus GR
62 GPa
Bulk Modulus KR
128 GPa
Shear Modulus GVRH
63 GPa
Bulk Modulus KVRH
129 GPa
Elastic Anisotropy
0.11
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CeMgCu2 (mp-22237) 0.7496 0.022 3
Al(CoSi)2 (mp-10010) 0.2581 0.000 3
UInPt2 (mp-1079904) 0.7457 0.174 3
Al3Ru2 (mp-1069983) 0.0877 0.238 2
Al3Cu2 (mp-10886) 0.1176 0.034 2
Ga3Pt2 (mp-21400) 0.1937 0.004 2
In3Pt2 (mp-1069815) 0.1256 0.005 2
Al3Pt2 (mp-10905) 0.1463 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Al Pd
Final Energy/Atom
-5.0922 eV
Corrected Energy
-25.4611 eV
Uncorrected energy = -25.4611 eV Corrected energy = -25.4611 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 58117
Submitted by
User remarks:
  • Aluminium palladium (3/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)