Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.777 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca(BeGe)2 (mp-31209) | 0.2503 | 0.026 | 3 |
Gd(CuSi)2 (mp-20677) | 0.2533 | 0.000 | 3 |
U(GeIr)2 (mp-1078742) | 0.2567 | 0.038 | 3 |
Sr(ZnSn)2 (mp-1080049) | 0.2264 | 0.000 | 3 |
Y(GePt)2 (mp-1084838) | 0.2481 | 0.009 | 3 |
La3Cu4(P2O)2 (mp-6309) | 0.6265 | 0.000 | 4 |
YbGa4 (mp-1088) | 0.2788 | 0.000 | 2 |
CaGa4 (mp-1976) | 0.2739 | 0.000 | 2 |
SrGa4 (mp-1827) | 0.2820 | 0.000 | 2 |
BaAl4 (mp-1903) | 0.2637 | 0.000 | 2 |
BaIn4 (mp-22687) | 0.2763 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Ge_d Pt |
Final Energy/Atom-5.4523 eV |
Corrected Energy-54.5226 eV
Uncorrected energy = -54.5226 eV
Corrected energy = -54.5226 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)