Mg(Co3P2)2

ID:

mp-10924

DOI:

10.17188/1187464


Tags: Magnesium cobalt phosphide (1/6/4)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.635 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.63 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P6m2 [187]
Hall
P 6 2
Point Group
6m2
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 94412 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnO (mp-2133) <0 0 1> <0 0 1> 0.004 37.4
AlN (mp-661) <1 0 1> <1 1 1> 0.004 53.5
Ni (mp-23) <1 1 1> <0 0 1> 0.005 149.6
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.010 112.2
CdSe (mp-2691) <1 0 0> <1 0 1> 0.012 347.4
GaSb (mp-1156) <1 0 0> <1 0 1> 0.016 347.4
LiAlO2 (mp-3427) <1 1 1> <1 0 1> 0.023 217.1
TePb (mp-19717) <1 1 0> <1 0 0> 0.027 242.8
CdWO4 (mp-19387) <1 1 1> <1 0 0> 0.030 154.5
PbSe (mp-2201) <1 0 0> <1 0 1> 0.030 347.4
SiC (mp-8062) <1 0 0> <1 0 1> 0.044 173.7
Al (mp-134) <1 1 1> <0 0 1> 0.046 112.2
AlN (mp-661) <1 1 0> <1 0 1> 0.056 217.1
BaTiO3 (mp-5986) <1 1 1> <1 1 0> 0.058 114.7
LiAlO2 (mp-3427) <0 0 1> <1 0 1> 0.066 217.1
GaN (mp-804) <1 1 1> <1 0 0> 0.066 242.8
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.067 261.8
ZnTe (mp-2176) <1 0 0> <1 0 1> 0.080 347.4
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.094 110.4
InAs (mp-20305) <1 0 0> <1 0 1> 0.097 347.4
InAs (mp-20305) <1 1 1> <0 0 1> 0.108 261.8
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.113 187.0
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.130 261.8
GaSe (mp-1943) <0 0 1> <0 0 1> 0.132 37.4
MgO (mp-1265) <1 0 0> <1 1 0> 0.133 344.1
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.134 154.5
SiO2 (mp-6930) <1 1 1> <1 0 1> 0.134 260.5
InSb (mp-20012) <1 0 0> <1 0 0> 0.155 44.1
Mg (mp-153) <1 1 1> <1 0 0> 0.156 242.8
CdTe (mp-406) <1 0 0> <1 0 0> 0.160 44.1
MoSe2 (mp-1634) <0 0 1> <1 1 0> 0.172 38.2
WSe2 (mp-1821) <0 0 1> <1 1 0> 0.172 38.2
GaAs (mp-2534) <1 1 0> <0 0 1> 0.174 187.0
ZnSe (mp-1190) <1 1 0> <0 0 1> 0.177 187.0
MgF2 (mp-1249) <1 0 1> <1 1 1> 0.192 53.5
Ge (mp-32) <1 1 0> <0 0 1> 0.195 187.0
CdS (mp-672) <0 0 1> <1 0 1> 0.196 217.1
Ni (mp-23) <1 0 0> <1 0 0> 0.196 198.6
MgF2 (mp-1249) <1 1 1> <1 1 0> 0.199 152.9
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.200 187.0
ZrO2 (mp-2858) <0 1 1> <1 0 0> 0.219 154.5
C (mp-48) <0 0 1> <1 0 0> 0.224 242.8
WSe2 (mp-1821) <1 0 0> <1 1 0> 0.225 152.9
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.226 187.0
TiO2 (mp-390) <0 0 1> <1 1 1> 0.241 213.9
LiF (mp-1138) <1 1 0> <0 0 1> 0.245 187.0
AlN (mp-661) <1 0 0> <1 0 0> 0.247 286.9
Mg (mp-153) <0 0 1> <0 0 1> 0.250 112.2
BN (mp-984) <0 0 1> <1 0 0> 0.250 242.8
CdWO4 (mp-19387) <1 1 0> <1 0 0> 0.251 242.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
350 121 146 0 0 0
121 350 146 0 0 0
146 146 300 0 0 0
0 0 0 95 0 0
0 0 0 0 95 0
0 0 0 0 0 114
Compliance Tensor Sij (10-12Pa-1)
3.7 -0.7 -1.5 0 0 0
-0.7 3.7 -1.5 0 0 0
-1.5 -1.5 4.8 0 0 0
0 0 0 10.6 0 0
0 0 0 0 10.6 0
0 0 0 0 0 8.7
Shear Modulus GV
100 GPa
Bulk Modulus KV
203 GPa
Shear Modulus GR
98 GPa
Bulk Modulus KR
203 GPa
Shear Modulus GVRH
99 GPa
Bulk Modulus KVRH
203 GPa
Elastic Anisotropy
0.09
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li(Co3P2)2 (mp-8864) 0.1727 0.000 3
Yb(As2Rh3)2 (mp-20082) 0.1452 0.000 3
Mg(P2Rh3)2 (mp-10440) 0.2459 0.016 3
Mg(As2Rh3)2 (mp-16043) 0.2418 0.009 3
Ca(As2Rh3)2 (mp-16044) 0.1537 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Co P
Final Energy/Atom
-6.6262 eV
Corrected Energy
-72.8882 eV
-72.8882 eV = -72.8882 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 94412
Submitted by
User remarks:
  • Magnesium cobalt phosphide (1/6/4)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)