Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.003 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.098 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density0.97 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaP + H2 |
Band Gap1.214 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li6Br3N (mp-34326) | 0.5713 | 0.033 | 3 |
AgPF6 (mp-34418) | 0.0432 | 0.000 | 3 |
AgAsF6 (mp-37153) | 0.2308 | 0.000 | 3 |
NaAsF6 (mp-1087215) | 0.4079 | 0.002 | 3 |
NaPF6 (mp-10474) | 0.1501 | 0.000 | 3 |
RhF6 (mp-1025250) | 0.3434 | 0.000 | 2 |
RuF6 (mp-1025168) | 0.3837 | 0.005 | 2 |
ReF6 (mp-1025374) | 0.3420 | 0.000 | 2 |
TcF6 (mp-1025373) | 0.3585 | 0.000 | 2 |
MoF6 (mp-558836) | 0.3355 | 0.005 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv P H |
Final Energy/Atom-3.2684 eV |
Corrected Energy-26.1473 eV
-26.1473 eV = -26.1473 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)