Final Magnetic Moment0.030 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.014 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.041 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.48 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaMg + La |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
GaCo2Ni (mp-20551) | 0.1697 | 0.080 | 3 |
ZnCu2Ni (mp-30593) | 0.1021 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.1935 | 0.034 | 3 |
GaFeNi2 (mp-1065359) | 0.1961 | 0.065 | 3 |
MnGaFe2 (mp-1065753) | 0.1419 | 0.038 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.1987 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3165 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.3641 | 0.193 | 4 |
MgIn3 (mp-973308) | 0.0212 | 0.024 | 2 |
Sm3Zn (mp-978828) | 0.0212 | 0.136 | 2 |
Na3Tl (mp-977403) | 0.0052 | 0.017 | 2 |
SbPt3 (mp-973354) | 0.0214 | 0.119 | 2 |
Li3Be (mp-975794) | 0.0255 | 0.242 | 2 |
In (mp-85) | 0.0266 | 0.037 | 1 |
Na (mp-974920) | 0.1118 | 0.013 | 1 |
Tl (mp-151) | 0.0999 | 0.011 | 1 |
La (mp-156) | 0.1064 | 0.001 | 1 |
Sn (mp-623511) | 0.1068 | 0.061 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Mg_pv |
Final Energy/Atom-4.1160 eV |
Corrected Energy-16.4639 eV
-16.4639 eV = -16.4639 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)