Final Magnetic Moment2.024 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.223 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.239 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.36 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg149Ti + Ti |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1076 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0392 | 0.034 | 3 |
LiCa6Ge (mp-12609) | 0.0103 | 0.183 | 3 |
GaFeNi2 (mp-1065359) | 0.0312 | 0.065 | 3 |
GaCo2Ni (mp-1018060) | 0.0055 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2098 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3552 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.3970 | 0.193 | 4 |
Sm3Tm (mp-978960) | 0.0017 | 0.019 | 2 |
Nd3Ho (mp-976418) | 0.0017 | 0.017 | 2 |
Ag3Pd (mp-985296) | 0.0017 | 0.000 | 2 |
Re3Mo (mp-974420) | 0.0017 | 0.135 | 2 |
Ti3Ag (mp-621131) | 0.0009 | 0.145 | 2 |
As (mp-1096826) | 0.0087 | 0.559 | 1 |
Sc (mp-36) | 0.0086 | 0.048 | 1 |
Hg (mp-753304) | 0.0079 | 0.012 | 1 |
Th (mp-37) | 0.0083 | 0.000 | 1 |
Dy (mp-10750) | 0.0077 | 0.021 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Ti_pv |
Final Energy/Atom-2.9506 eV |
Corrected Energy-11.8023 eV
-11.8023 eV = -11.8023 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)