Final Magnetic Moment0.042 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.177 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.272 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.13 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSrMg2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6m2 [187] |
HallP 6 2 |
Point Group6m2 |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KNbSe2 (mp-7940) | 0.5341 | 0.029 | 3 |
KNbS2 (mp-7938) | 0.5547 | 0.009 | 3 |
NbInSe2 (mp-1018116) | 0.4540 | 0.004 | 3 |
InMoS2 (mp-1087488) | 0.7497 | 0.091 | 3 |
NbInS2 (mp-20621) | 0.5841 | 0.016 | 3 |
SrMg (mp-1094327) | 0.4541 | 0.205 | 2 |
Re3N (mp-974435) | 0.5385 | 0.000 | 2 |
Tc3N (mp-1017987) | 0.5431 | 0.000 | 2 |
Ag2F (mp-1391) | 0.6480 | 0.000 | 2 |
SrMg2 (mp-1094282) | 0.4430 | 0.275 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv Mg_pv |
Final Energy/Atom-1.4507 eV |
Corrected Energy-8.7044 eV
Uncorrected energy = -8.7044 eV
Corrected energy = -8.7044 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)