Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.035 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.024 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.22 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMg |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinAmm2 [38] |
HallA 2 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr8Ni50Mo15W2 (mp-767372) | 0.3441 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.1872 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.3510 | 0.193 | 4 |
Sm5Mg (mp-981747) | 0.0708 | 0.073 | 2 |
MgZn (mp-1094474) | 0.0797 | 0.093 | 2 |
MgSn2 (mp-1094234) | 0.0910 | 0.107 | 2 |
MgSb2 (mp-1094545) | 0.0961 | 0.240 | 2 |
K (mp-972981) | 0.2143 | 0.008 | 1 |
Y (mp-1059189) | 0.2195 | 0.004 | 1 |
Er (mp-99) | 0.2484 | 0.007 | 1 |
Ho (mp-144) | 0.2484 | 0.010 | 1 |
Pr (mp-1009594) | 0.2342 | 0.032 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Mg_pv |
Final Energy/Atom-1.7901 eV |
Corrected Energy-10.7404 eV
-10.7404 eV = -10.7404 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)