Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.015 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg17Al12 + Mg149Al |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na(Mg4Al3)4 (mp-976925) | 0.1622 | 0.016 | 3 |
Li(Mg4Al3)4 (mp-973924) | 0.1456 | 0.004 | 3 |
Li(Mg4Al3)4 (mp-973970) | 0.2594 | 0.008 | 3 |
Mg17Al11Pd (mp-865352) | 0.1930 | 0.010 | 3 |
Mg17Al11Ag (mp-865489) | 0.1361 | 0.006 | 3 |
Mg17Al12 (mp-2151) | 0.2340 | 0.000 | 2 |
Re24Mo5 (mp-12662) | 0.3941 | 0.000 | 2 |
Mg16Al13 (mp-1094683) | 0.2401 | 0.010 | 2 |
Mg16Al13 (mp-1094685) | 0.1050 | 0.004 | 2 |
Mg16Al13 (mp-1094692) | 0.1803 | 0.008 | 2 |
Mn (mp-35) | 0.4498 | 0.000 | 1 |
Hg (mp-864900) | 0.3668 | 0.001 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Al |
Final Energy/Atom-2.4294 eV |
Corrected Energy-70.4527 eV
-70.4527 eV = -70.4527 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)