Final Magnetic Moment0.175 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.012 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.025 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.50 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCeMg3 + Ce |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgTa (mp-978258) | 0.4544 | 0.336 | 2 |
Nb3Fe (mp-1067714) | 0.5841 | 0.264 | 2 |
YSn3 (mp-1094248) | 0.5843 | 0.066 | 2 |
CeMg (mp-1094963) | 0.2410 | 0.029 | 2 |
CeMg2 (mp-1039345) | 0.5392 | 0.005 | 2 |
Cr (mp-1059289) | 0.5018 | 0.336 | 1 |
Ga (mp-140) | 0.5858 | 0.024 | 1 |
Sb (mp-10631) | 0.6711 | 0.302 | 1 |
U (mp-44) | 0.6729 | 0.000 | 1 |
Ce (mp-64) | 0.4401 | 0.040 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce Mg_pv |
Final Energy/Atom-4.4768 eV |
Corrected Energy-26.8608 eV
-26.8608 eV = -26.8608 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)