Final Magnetic Moment14.013 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.880 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2InPt2 (mp-21885) | 0.1345 | 0.000 | 3 |
Ca2InPd2 (mp-20792) | 0.1578 | 0.000 | 3 |
Sr2InPd2 (mp-20843) | 0.2234 | 0.000 | 3 |
Ca2GaPt2 (mp-1078428) | 0.2755 | 0.000 | 3 |
Eu2InPd2 (mp-1095160) | 0.1051 | 0.000 | 3 |
Rb8In11 (mp-640712) | 0.6891 | 0.000 | 2 |
CeAl (mp-20439) | 0.6645 | 0.015 | 2 |
Rb8Tl11 (mp-542781) | 0.6880 | 0.000 | 2 |
K8In11 (mp-582929) | 0.6852 | 0.000 | 2 |
Mg3Si2 (mp-1075810) | 0.6831 | 0.120 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Eu In_d Pt |
Final Energy/Atom-7.9758 eV |
Corrected Energy-79.7582 eV
-79.7582 eV = -79.7582 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)