Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.467 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToWBr6 + WBr2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VOF3 (mp-764398) | 0.5494 | 0.058 | 3 |
NbSeCl9 (mp-29968) | 0.5800 | 0.004 | 3 |
Zr2TeBr12 (mp-28672) | 0.5145 | 0.000 | 3 |
Mo(SeCl6)2 (mp-568726) | 0.5350 | 0.032 | 3 |
NbTeCl9 (mp-669348) | 0.5863 | 0.003 | 3 |
RbAsOF4 (mp-17337) | 0.6494 | 0.000 | 4 |
KAsOF4 (mp-17539) | 0.6860 | 0.000 | 4 |
CsAsOF4 (mp-562403) | 0.6691 | 0.000 | 4 |
Te3As2(SF4)3 (mp-662789) | 0.7222 | 0.087 | 4 |
AsS3(ClF2)3 (mp-562439) | 0.7342 | 0.044 | 4 |
MoCl5 (mp-29147) | 0.1230 | 0.019 | 2 |
PaBr5 (mp-27642) | 0.1298 | 0.000 | 2 |
MoCl5 (mp-569436) | 0.0993 | 0.003 | 2 |
WBr5 (mp-29554) | 0.0680 | 0.012 | 2 |
MoCl5 (mp-571256) | 0.1191 | 0.003 | 2 |
FeH2C4N4Cl6O (mp-743856) | 0.7312 | 1.272 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: W_pv Br |
Final Energy/Atom-3.9903 eV |
Corrected Energy-47.8836 eV
-47.8836 eV = -47.8836 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)