@article{Mueller2010, author = "Mueller, C.J. and Schwarz, U. and Schmidt, P. and Schnelle, W. and Doert, T.", title = "High-pressure synthesis, crystal structure, and properties of Gd S2 with thermodynamic investigations in the phase diagram Gd - S", journal = "Zeitschrift fuer Anorganische und Allgemeine Chemie (1950) (DE)", year = "2010", volume = "636", pages = "947-953", ASTM_id = "ZAACAB" }