Final Magnetic Moment0.027 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.436 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.436 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn + Nd |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 26.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 214.1 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 138.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 92.1 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 239.3 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 239.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 321.2 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 230.3 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 252.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 187.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 213.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 138.2 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 230.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 230.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 319.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 168.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 230.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 239.3 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 230.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 80.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 46.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 26.8 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 230.3 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 213.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 138.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 230.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 230.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 348.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 160.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 53.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 184.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 187.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 138.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 187.4 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 184.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 26.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 107.1 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 239.3 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 276.4 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 239.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 348.0 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 214.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 276.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 138.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 138.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 321.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 294.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 348.0 |
BN (mp-984) | <1 0 1> | <1 0 0> | 138.2 |
BN (mp-984) | <1 1 1> | <1 1 0> | 239.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2Mg3Si (mp-1095343) | 0.1935 | 0.119 | 3 |
Eu2Ga3Ir (mp-609413) | 0.2002 | 0.000 | 3 |
Er2Al3Co (mp-567849) | 0.1699 | 0.000 | 3 |
Nb2Co3Si (mp-10366) | 0.2549 | 0.000 | 3 |
Lu2Al3Co (mp-16490) | 0.1856 | 0.000 | 3 |
TmMn2 (mp-30786) | 0.2020 | 0.033 | 2 |
SrZn2 (mp-13365) | 0.1964 | 0.049 | 2 |
ErMn2 (mp-913259) | 0.2225 | 0.042 | 2 |
SmMn2 (mp-1095689) | 0.0984 | 0.148 | 2 |
NdMn2 (mp-569334) | 0.1445 | 0.436 | 2 |
Co (mp-1072089) | 0.4241 | 0.199 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 Mn_pv |
Final Energy/Atom-7.2610 eV |
Corrected Energy-87.1320 eV
-87.1320 eV = -87.1320 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)