Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.756 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.111 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SmAsS (mp-557569) | 0.0969 | 0.001 | 3 |
YAsSe (mp-1095603) | 0.3793 | 0.000 | 3 |
CeAsS (mp-1095615) | 0.2433 | 0.034 | 3 |
LuAsSe (mp-1095656) | 0.3655 | 0.000 | 3 |
CeAsS (mp-1095675) | 0.1840 | 0.000 | 3 |
ThAs2 (mp-7097) | 0.6371 | 0.000 | 2 |
ThSb2 (mp-7568) | 0.6168 | 0.000 | 2 |
YbSe2 (mp-1077033) | 0.5148 | 0.184 | 2 |
YbTe2 (mp-1077459) | 0.5154 | 0.120 | 2 |
YbS2 (mp-1076966) | 0.5216 | 0.254 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Er_3 As S |
Final Energy/Atom-5.9888 eV |
Corrected Energy-74.5196 eV
-74.5196 eV = -71.8658 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)