@article{Baldinozzi2002, author = "Baldinozzi, G. and Malinowska, B. and Rakib, M. and Durand, G.", title = "Crystal structure and characterisation of cadmium cyanamide", journal = "Journal of Materials Chemistry", year = "2002", volume = "12", pages = "268-272", ASTM_id = "JMACEP" }