Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.308 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.99 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 52124 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Te2W (mp-22693) <0 0 1> <0 1 1> 0.001 110.7
SiC (mp-7631) <1 1 0> <0 0 1> 0.002 244.2
InAs (mp-20305) <1 0 0> <0 1 0> 0.003 305.1
ZnTe (mp-2176) <1 0 0> <0 1 0> 0.007 305.1
TiO2 (mp-390) <1 1 0> <1 0 0> 0.018 156.2
SrTiO3 (mp-4651) <1 0 0> <0 1 1> 0.025 221.5
MgAl2O4 (mp-3536) <1 1 0> <0 1 0> 0.026 284.7
SrTiO3 (mp-4651) <0 0 1> <0 1 1> 0.026 249.2
SiC (mp-11714) <1 1 1> <1 0 1> 0.028 109.3
LiTaO3 (mp-3666) <1 0 1> <0 1 0> 0.031 305.1
DyScO3 (mp-31120) <1 1 1> <1 0 0> 0.033 281.1
ZrO2 (mp-2858) <1 1 -1> <0 1 0> 0.036 183.0
SiC (mp-11714) <1 1 0> <1 0 1> 0.037 109.3
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.040 93.7
GdScO3 (mp-5690) <1 0 0> <1 0 0> 0.049 93.7
TiO2 (mp-390) <1 1 1> <1 0 1> 0.053 109.3
Ga2O3 (mp-886) <1 0 -1> <0 1 0> 0.055 305.1
SrTiO3 (mp-4651) <1 1 1> <0 1 1> 0.056 138.4
WS2 (mp-224) <1 0 1> <1 1 0> 0.056 186.4
YAlO3 (mp-3792) <1 0 1> <1 0 1> 0.056 145.8
CdWO4 (mp-19387) <0 1 1> <1 0 0> 0.058 281.1
SiO2 (mp-6930) <1 0 1> <0 1 0> 0.068 244.0
WSe2 (mp-1821) <1 1 0> <1 1 0> 0.069 260.9
LaF3 (mp-905) <1 0 0> <0 0 1> 0.070 319.3
Ga2O3 (mp-886) <0 1 0> <0 1 0> 0.070 142.4
SiC (mp-11714) <0 0 1> <0 0 1> 0.072 131.5
TeO2 (mp-2125) <1 0 0> <0 1 0> 0.073 142.4
TbScO3 (mp-31119) <1 1 1> <1 0 0> 0.073 281.1
TbScO3 (mp-31119) <1 0 1> <1 1 0> 0.074 111.8
TeO2 (mp-2125) <1 0 1> <1 0 0> 0.077 156.2
SiC (mp-7631) <0 0 1> <0 0 1> 0.079 131.5
DyScO3 (mp-31120) <1 0 1> <1 1 0> 0.084 111.8
TeO2 (mp-2125) <0 1 1> <0 1 0> 0.084 305.1
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.087 187.8
GaAs (mp-2534) <1 1 0> <1 0 0> 0.087 93.7
AlN (mp-661) <1 1 1> <0 0 1> 0.091 56.3
CdSe (mp-2691) <1 0 0> <0 1 0> 0.092 305.1
ZnSe (mp-1190) <1 1 0> <1 0 0> 0.094 93.7
Ge (mp-32) <1 1 0> <1 0 0> 0.095 93.7
TeO2 (mp-2125) <0 0 1> <0 1 0> 0.095 162.7
MgO (mp-1265) <1 1 1> <0 1 1> 0.098 221.5
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.102 186.4
KCl (mp-23193) <1 1 0> <1 1 1> 0.114 292.2
Ge3(BiO3)4 (mp-23560) <1 0 0> <0 0 1> 0.119 112.7
LiF (mp-1138) <1 1 0> <1 0 0> 0.124 93.7
GaSb (mp-1156) <1 0 0> <0 1 0> 0.125 305.1
KP(HO2)2 (mp-23959) <0 0 1> <0 0 1> 0.126 75.1
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.127 56.3
InAs (mp-20305) <1 1 1> <1 0 1> 0.129 328.0
AlN (mp-661) <1 1 0> <1 0 1> 0.130 109.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
203 94 131 0 0 0
94 180 109 0 0 0
131 109 178 0 0 0
0 0 0 70 0 0
0 0 0 0 103 0
0 0 0 0 0 101
Compliance Tensor Sij (10-12Pa-1)
9.6 -1.2 -6.3 0 0 0
-1.2 9 -4.6 0 0 0
-6.3 -4.6 13.1 0 0 0
0 0 0 14.3 0 0
0 0 0 0 9.7 0
0 0 0 0 0 9.9
Shear Modulus GV
70 GPa
Bulk Modulus KV
137 GPa
Shear Modulus GR
54 GPa
Bulk Modulus KR
135 GPa
Shear Modulus GVRH
62 GPa
Bulk Modulus KVRH
136 GPa
Elastic Anisotropy
1.47
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
AsRh (mp-22079) 0.1459 0.004 2
MnAs (mp-22240) 0.2010 0.018 2
CoP (mp-22270) 0.1699 0.000 2
CoAs (mp-583) 0.1731 0.000 2
MnAs (mp-612701) 0.1731 0.018 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ni_pv Ge_d
Final Energy/Atom
-5.5066 eV
Corrected Energy
-44.0524 eV
-44.0524 eV = -44.0524 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 52124
  • 659794
  • 76623
Submitted by
User remarks:
  • Nickel germanide (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)