Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.958 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPrTe3 + K2Te3 + KPr3Te8 |
Band Gap0.183 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/nbm [125] |
HallP 4 2 1ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 0> | 314.6 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 251.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 242.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 291.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 194.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 242.9 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 238.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 340.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 251.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 177.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 266.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 291.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 194.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 145.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 251.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 314.6 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 238.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 340.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 340.1 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 188.7 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 125.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 340.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 251.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 194.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 242.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 291.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 202.8 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 251.7 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 251.7 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 238.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 145.8 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 314.6 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 266.9 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 188.7 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 125.8 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 177.9 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 314.6 |
C (mp-66) | <1 1 1> | <1 1 0> | 89.0 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 242.9 |
LiNbO3 (mp-3731) | <1 1 1> | <1 1 0> | 266.9 |
Al (mp-134) | <1 1 0> | <1 0 0> | 314.6 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 242.9 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 0> | 266.9 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 291.5 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 242.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 251.7 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 242.9 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 0> | 266.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 242.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 194.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
51 | 30 | 10 | 0 | 0 | 0 |
30 | 51 | 10 | 0 | 0 | 0 |
10 | 10 | 31 | 0 | 0 | 0 |
0 | 0 | 0 | 9 | 0 | 0 |
0 | 0 | 0 | 0 | 9 | 0 |
0 | 0 | 0 | 0 | 0 | 34 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
31.4 | -17.8 | -4.5 | 0 | 0 | 0.0 |
-17.8 | 31.4 | -4.5 | 0 | 0 | -0.0 |
-4.5 | -4.5 | 35.6 | 0 | 0 | 0.0 |
0 | 0 | 0 | 109.3 | 0 | 0 |
0 | 0 | 0 | 0 | 109.3 | 0 |
0.0 | -0.0 | 0 | 0 | 0 | 29.6 |
Shear Modulus GV16 GPa |
Bulk Modulus KV26 GPa |
Shear Modulus GR12 GPa |
Bulk Modulus KR22 GPa |
Shear Modulus GVRH14 GPa |
Bulk Modulus KVRH24 GPa |
Elastic Anisotropy1.72 |
Poisson's Ratio0.26 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RbPrTe4 (mp-7199) | 0.2362 | 0.000 | 3 |
KGdTe4 (mp-542281) | 0.1272 | 0.000 | 3 |
KNdTe4 (mp-11010) | 0.0527 | 0.004 | 3 |
RbNdTe4 (mp-11011) | 0.2648 | 0.003 | 3 |
KCeSe4 (mp-22395) | 0.1857 | 0.012 | 3 |
PbSe2 (mp-982261) | 0.6048 | 0.054 | 2 |
Mg2Si (mp-1074753) | 0.5506 | 0.131 | 2 |
BaTe2 (mp-2150) | 0.5165 | 0.002 | 2 |
SrS2 (mp-1950) | 0.6806 | 0.011 | 2 |
Mg4Si3 (mp-1078478) | 0.6936 | 0.260 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Pr_3 Te |
Final Energy/Atom-4.0355 eV |
Corrected Energy-48.4260 eV
-48.4260 eV = -48.4260 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)