Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.191 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mcm [140] |
Hall-I 4 2c |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 270.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 67.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 96.4 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 117.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 235.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 289.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 270.5 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 289.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 135.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 192.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 235.6 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 117.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 289.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 67.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 67.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 96.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 270.5 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 270.5 |
TePb (mp-19717) | <1 1 1> | <1 0 1> | 235.6 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 96.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 270.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 96.4 |
BN (mp-984) | <0 0 1> | <1 0 1> | 235.6 |
BN (mp-984) | <1 1 1> | <1 0 1> | 235.6 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 135.2 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 192.9 |
CdTe (mp-406) | <1 1 1> | <1 0 1> | 235.6 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 289.3 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 202.8 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 289.3 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 289.3 |
TiO2 (mp-2657) | <1 0 1> | <1 0 1> | 235.6 |
C (mp-66) | <1 0 0> | <1 0 0> | 192.9 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 96.4 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 67.6 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 270.5 |
C (mp-66) | <1 1 0> | <1 0 0> | 289.3 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 135.2 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 289.3 |
InP (mp-20351) | <1 1 1> | <1 0 1> | 117.8 |
Mg (mp-153) | <0 0 1> | <1 0 1> | 235.6 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 202.8 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 192.9 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 192.9 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 192.9 |
InSb (mp-20012) | <1 1 1> | <1 0 1> | 235.6 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 96.4 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 67.6 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 270.5 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 96.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaFe9Si4 (mp-662529) | 0.1846 | 0.019 | 3 |
CeGa4Co9 (mp-1006277) | 0.2103 | 0.017 | 3 |
SrCu9Si4 (mp-11142) | 0.0690 | 0.000 | 3 |
SrCu9Ge4 (mp-11144) | 0.2303 | 0.000 | 3 |
BaCu9Ge4 (mp-11145) | 0.2140 | 0.000 | 3 |
ZrBe13 (mp-30445) | 0.3364 | 0.000 | 2 |
LaCo13 (mp-30559) | 0.3116 | 0.000 | 2 |
RbZn13 (mp-2504) | 0.3391 | 0.000 | 2 |
HfBe13 (mp-1878) | 0.3274 | 0.000 | 2 |
UBe13 (mp-1163) | 0.3299 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Cu_pv Si |
Final Energy/Atom-4.5138 eV |
Corrected Energy-126.3873 eV
-126.3873 eV = -126.3873 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)