material

LiZnPS4

ID:

mp-11175

DOI:

10.17188/1187611


Tags: Lithium zinc thiophosphate(V)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.039 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.50 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.929 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4 [82]
Hall
I 4
Point Group
4
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 95785 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InAs (mp-20305) <1 0 0> <0 0 1> 0.002 304.9
GaTe (mp-542812) <1 0 0> <1 0 1> 0.002 314.1
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.003 304.9
Cu (mp-30) <1 0 0> <0 0 1> 0.003 169.4
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.004 304.9
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.006 135.5
Mg (mp-153) <1 1 1> <0 0 1> 0.008 271.0
LiAlO2 (mp-3427) <1 0 1> <1 1 0> 0.009 299.3
Si (mp-149) <1 0 0> <0 0 1> 0.010 271.0
Mg (mp-153) <1 0 1> <1 0 1> 0.010 188.5
GaP (mp-2490) <1 0 0> <0 0 1> 0.010 271.0
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.011 271.0
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.012 271.0
GdScO3 (mp-5690) <1 0 1> <0 0 1> 0.013 169.4
LiGaO2 (mp-5854) <0 0 1> <1 0 1> 0.013 251.3
ZnO (mp-2133) <1 0 1> <1 1 0> 0.014 299.3
Mg (mp-153) <1 1 0> <1 0 0> 0.017 317.5
Ni (mp-23) <1 0 0> <0 0 1> 0.018 304.9
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.019 135.5
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.021 304.9
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.024 271.0
Ge (mp-32) <1 1 0> <1 0 1> 0.028 188.5
GaTe (mp-542812) <1 0 -1> <0 0 1> 0.030 304.9
BN (mp-984) <0 0 1> <1 1 0> 0.032 224.5
TbScO3 (mp-31119) <1 0 1> <0 0 1> 0.033 169.4
CdSe (mp-2691) <1 0 0> <0 0 1> 0.036 304.9
CsI (mp-614603) <1 0 0> <0 0 1> 0.036 304.9
GaN (mp-804) <1 1 0> <1 0 0> 0.037 317.5
GaAs (mp-2534) <1 1 0> <1 0 1> 0.039 188.5
ZrO2 (mp-2858) <1 0 1> <1 1 0> 0.040 299.3
Ag (mp-124) <1 1 1> <0 0 1> 0.042 237.1
Ag (mp-124) <1 1 0> <0 0 1> 0.042 169.4
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.043 264.6
TeO2 (mp-2125) <1 0 0> <1 0 0> 0.045 211.7
MgAl2O4 (mp-3536) <1 0 0> <0 0 1> 0.046 67.8
GaSb (mp-1156) <1 0 0> <0 0 1> 0.048 304.9
ZnSe (mp-1190) <1 1 0> <1 0 1> 0.050 188.5
LiAlO2 (mp-3427) <1 0 0> <1 1 1> 0.050 164.3
DyScO3 (mp-31120) <0 0 1> <1 0 1> 0.052 62.8
LiF (mp-1138) <1 0 0> <0 0 1> 0.052 33.9
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.055 251.3
GdScO3 (mp-5690) <1 0 0> <1 0 1> 0.056 188.5
NdGaO3 (mp-3196) <0 1 1> <1 0 1> 0.059 314.1
DyScO3 (mp-31120) <1 0 1> <0 0 1> 0.061 169.4
WSe2 (mp-1821) <1 1 0> <1 0 0> 0.061 264.6
CdWO4 (mp-19387) <1 1 0> <0 0 1> 0.064 203.3
TbScO3 (mp-31119) <0 0 1> <1 0 1> 0.064 62.8
CdWO4 (mp-19387) <1 1 1> <1 0 1> 0.065 314.1
PbSe (mp-2201) <1 0 0> <0 0 1> 0.065 304.9
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.070 135.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
49 14 26 0 0 3
14 49 26 0 0 -3
26 26 43 0 0 0
0 0 0 22 0 0
0 0 0 0 22 0
3 -3 0 0 0 16
Compliance Tensor Sij (10-12Pa-1)
31.3 1.2 -19.7 0 0 -5.5
1.2 31.3 -19.7 0 0 5.5
-19.7 -19.7 46.9 0 0 0
0 0 0 45.8 0 0
0 0 0 0 45.8 0
-5.5 5.5 0 0 0 64.6
Shear Modulus GV
17 GPa
Bulk Modulus KV
31 GPa
Shear Modulus GR
14 GPa
Bulk Modulus KR
30 GPa
Shear Modulus GVRH
16 GPa
Bulk Modulus KVRH
30 GPa
Elastic Anisotropy
0.95
Poisson's Ratio
0.28

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.01492 0.03219 0.00000
0.00000 0.00000 0.00000 -0.03219 0.01492 0.00000
0.01578 -0.01578 0.00000 0.00000 0.00000 -0.18513
Piezoelectric Modulus ‖eijmax
0.18647 C/m2
Crystallographic Direction vmax
0.00000
0.00000
1.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.71 0.00 0.00
-0.00 4.71 0.00
0.00 0.00 4.86
Dielectric Tensor εij (total)
7.63 0.00 0.00
-0.00 7.63 0.00
0.00 0.00 8.12
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.76
Polycrystalline dielectric constant εpoly
(total)
7.79
Refractive Index n
2.18
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Al2CdS4 (mp-5928) 0.4228 0.000 3
Al2HgS4 (mp-7906) 0.4236 0.000 3
Li2CrO4 (mp-769767) 0.3589 0.020 3
Li2FeF4 (mp-777130) 0.4081 0.350 3
Li2MnF4 (mp-763098) 0.3355 0.093 3
LiCoSiO4 (mp-762221) 0.3725 0.078 4
LiFeSiO4 (mp-767850) 0.3872 0.052 4
LiVSiO4 (mp-767069) 0.3055 0.086 4
LiFeSiO4 (mp-762631) 0.3835 0.079 4
LiGeBO4 (mp-8873) 0.3910 0.000 4
CuS2 (mp-684604) 0.6235 0.100 2
C3N4 (mp-571653) 0.5549 0.484 2
B2O (mp-614006) 0.6005 0.925 2
CN2 (mp-1019086) 0.6047 0.358 2
SiC2 (mp-1019097) 0.6088 0.562 2
Li4Ga3Si3IO12 (mp-557112) 0.5635 0.000 5
Li4Al3Ge3IO12 (mp-557456) 0.6370 0.000 5
Li4Ga3Si3ClO12 (mp-554203) 0.6348 0.000 5
Li4Ga3Si3BrO12 (mp-556649) 0.6096 0.000 5
Mn4Be3Ge3SeO12 (mp-25766) 0.6580 0.000 5
C (mp-568410) 0.7482 0.507 1
C (mp-1008374) 0.6862 0.437 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv Zn P S
Final Energy/Atom
-4.2497 eV
Corrected Energy
-32.4020 eV
-32.4020 eV = -29.7482 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 95785
Submitted by
User remarks:
  • Lithium zinc thiophosphate(V)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)