material

Al12W

ID:

mp-11227

DOI:

10.17188/1187650


Tags: Aluminum tungsten (12/1)

Material Details

Final Magnetic Moment
0.005 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.081 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.86 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Im3 [204]
Hall
-I 2 2 3
Point Group
m3
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 58207 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-8062) <1 1 1> <1 1 1> 0.000 99.7
SiC (mp-8062) <1 1 0> <1 1 0> 0.000 81.4
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.001 287.9
PbS (mp-21276) <1 0 0> <1 0 0> 0.001 287.9
C (mp-66) <1 1 0> <1 1 0> 0.001 162.9
C (mp-66) <1 0 0> <1 0 0> 0.001 115.2
TePb (mp-19717) <1 1 1> <1 1 1> 0.002 299.2
TePb (mp-19717) <1 1 0> <1 1 0> 0.002 244.3
SiC (mp-7631) <0 0 1> <1 1 1> 0.002 99.7
SiC (mp-11714) <0 0 1> <1 1 1> 0.004 99.7
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.008 162.9
C (mp-48) <0 0 1> <1 1 1> 0.011 99.7
InAs (mp-20305) <1 1 0> <1 1 0> 0.013 162.9
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.016 287.9
CdSe (mp-2691) <1 1 0> <1 1 0> 0.017 162.9
TiO2 (mp-390) <0 0 1> <1 0 0> 0.023 57.6
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.027 299.2
KP(HO2)2 (mp-23959) <0 1 0> <1 0 0> 0.027 230.3
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.028 299.2
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.028 299.2
GaSb (mp-1156) <1 1 0> <1 1 0> 0.032 162.9
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.033 287.9
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.043 115.2
PbSe (mp-2201) <1 1 0> <1 1 0> 0.058 162.9
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.078 287.9
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.090 244.3
NaCl (mp-22862) <1 0 0> <1 0 0> 0.092 287.9
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 1 0> 0.095 162.9
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 0> 0.095 115.2
LaAlO3 (mp-2920) <1 0 1> <1 1 1> 0.096 299.2
KP(HO2)2 (mp-23959) <0 0 1> <1 0 0> 0.098 230.3
ZnO (mp-2133) <1 1 0> <1 1 0> 0.100 244.3
Te2Mo (mp-602) <1 0 0> <1 1 0> 0.102 162.9
InP (mp-20351) <1 0 0> <1 0 0> 0.116 287.9
LiF (mp-1138) <1 0 0> <1 0 0> 0.140 287.9
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.144 287.9
Cu (mp-30) <1 1 1> <1 1 1> 0.146 299.2
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.168 99.7
CdTe (mp-406) <1 1 1> <1 1 1> 0.177 299.2
CdTe (mp-406) <1 1 0> <1 1 0> 0.177 244.3
LiGaO2 (mp-5854) <1 1 0> <1 1 0> 0.188 244.3
Au (mp-81) <1 0 0> <1 0 0> 0.189 230.3
BN (mp-984) <1 0 0> <1 0 0> 0.200 57.6
InSb (mp-20012) <1 1 1> <1 1 1> 0.204 299.2
InSb (mp-20012) <1 1 0> <1 1 0> 0.204 244.3
DyScO3 (mp-31120) <0 1 0> <1 0 0> 0.217 172.8
LaAlO3 (mp-2920) <1 0 0> <1 0 0> 0.227 287.9
Al (mp-134) <1 0 0> <1 0 0> 0.228 287.9
TeO2 (mp-2125) <0 0 1> <1 0 0> 0.229 287.9
YAlO3 (mp-3792) <1 0 0> <1 1 0> 0.250 81.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
168 53 53 0 0 0
53 168 53 0 0 0
53 53 168 0 0 0
0 0 0 56 0 0
0 0 0 0 56 0
0 0 0 0 0 56
Compliance Tensor Sij (10-12Pa-1)
7 -1.7 -1.7 0 0 0
-1.7 7 -1.7 0 0 0
-1.7 -1.7 7 0 0 0
0 0 0 17.8 0 0
0 0 0 0 17.8 0
0 0 0 0 0 17.8
Shear Modulus GV
57 GPa
Bulk Modulus KV
92 GPa
Shear Modulus GR
57 GPa
Bulk Modulus KR
92 GPa
Shear Modulus GVRH
57 GPa
Bulk Modulus KVRH
92 GPa
Elastic Anisotropy
0.00
Poisson's Ratio
0.24

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Al12Mo (mp-550) 0.0082 0.011 2
Al12Tc (mp-16719) 0.0200 0.000 2
Al12Re (mp-1648) 0.0210 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Al W_pv
Final Energy/Atom
-4.5352 eV
Corrected Energy
-58.9575 eV
Uncorrected energy = -58.9575 eV Corrected energy = -58.9575 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 58207
Submitted by
User remarks:
  • Aluminum tungsten (12/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)