material

YAl

ID:

mp-11228

DOI:

10.17188/1187651


Tags: Yttrium aluminium (1/1) Aluminium yttrium (1/1) Aluminum yttrium (1/1)

Material Details

Final Magnetic Moment
0.253 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.418 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.005 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.88 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Y2Al + YAl2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmcm [63]
Hall
-C 2c 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 58209 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GdScO3 (mp-5690) <0 0 1> <0 1 0> 0.001 255.4
Ga2O3 (mp-886) <1 0 -1> <0 1 1> 0.002 191.9
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.003 89.7
Si (mp-149) <1 0 0> <0 0 1> 0.003 89.7
GaN (mp-804) <1 0 0> <0 1 1> 0.021 287.8
TbScO3 (mp-31119) <1 0 1> <0 0 1> 0.023 224.3
MgAl2O4 (mp-3536) <1 0 0> <0 0 1> 0.026 134.6
DyScO3 (mp-31120) <1 0 1> <0 0 1> 0.036 224.3
TiO2 (mp-2657) <1 1 1> <0 1 0> 0.039 204.3
Cu (mp-30) <1 1 1> <0 1 0> 0.041 68.1
BaF2 (mp-1029) <1 1 1> <0 1 0> 0.049 68.1
YVO4 (mp-19133) <1 0 0> <0 1 0> 0.051 323.4
SrTiO3 (mp-4651) <1 0 1> <0 1 0> 0.057 323.4
SiC (mp-8062) <1 1 0> <1 1 0> 0.057 54.0
Ag (mp-124) <1 1 1> <0 1 0> 0.063 119.2
C (mp-48) <0 0 1> <0 1 0> 0.064 68.1
BN (mp-984) <1 0 0> <0 1 1> 0.065 95.9
Fe2O3 (mp-24972) <0 0 1> <0 1 0> 0.068 68.1
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.071 314.0
GdScO3 (mp-5690) <1 0 1> <0 0 1> 0.073 224.3
Ga2O3 (mp-886) <0 1 0> <1 1 0> 0.087 216.1
TbScO3 (mp-31119) <0 0 1> <0 1 0> 0.088 255.4
LaF3 (mp-905) <1 0 0> <0 0 1> 0.092 269.1
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.098 162.1
GaN (mp-804) <1 1 0> <0 1 0> 0.103 323.4
C (mp-48) <1 0 0> <0 1 1> 0.105 95.9
Al2O3 (mp-1143) <1 0 0> <0 1 0> 0.109 255.4
GaSe (mp-1943) <0 0 1> <0 1 0> 0.120 51.1
Au (mp-81) <1 1 1> <0 1 0> 0.120 119.2
Ag (mp-124) <1 0 0> <1 0 1> 0.121 68.1
GaSe (mp-1943) <1 0 0> <0 1 0> 0.121 68.1
NdGaO3 (mp-3196) <1 0 1> <0 1 0> 0.121 323.4
Mg (mp-153) <1 0 1> <0 0 1> 0.127 224.3
CdWO4 (mp-19387) <1 0 1> <1 1 0> 0.128 270.1
BaTiO3 (mp-5986) <1 1 1> <0 1 0> 0.128 289.4
GaP (mp-2490) <1 0 0> <0 0 1> 0.129 89.7
ZrO2 (mp-2858) <0 1 0> <0 1 0> 0.130 306.4
TiO2 (mp-2657) <0 0 1> <0 1 1> 0.139 239.9
AlN (mp-661) <1 1 1> <1 1 1> 0.149 140.4
PbSe (mp-2201) <1 1 1> <0 1 0> 0.156 68.1
AlN (mp-661) <1 0 1> <1 1 1> 0.157 70.2
NaCl (mp-22862) <1 1 1> <0 1 0> 0.161 221.3
ZrO2 (mp-2858) <1 1 -1> <1 1 0> 0.163 270.1
SiC (mp-11714) <0 0 1> <0 1 0> 0.168 204.3
NdGaO3 (mp-3196) <1 0 0> <0 1 0> 0.170 306.4
WSe2 (mp-1821) <0 0 1> <0 1 0> 0.170 68.1
MoSe2 (mp-1634) <0 0 1> <0 1 0> 0.171 68.1
CdWO4 (mp-19387) <1 1 0> <1 0 1> 0.172 204.4
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.175 134.6
SiC (mp-7631) <0 0 1> <0 1 0> 0.178 204.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
127 30 52 0 0 0
30 133 49 0 0 0
52 49 56 0 0 0
0 0 0 36 0 0
0 0 0 0 67 0
0 0 0 0 0 49
Compliance Tensor Sij (10-12Pa-1)
13.3 2.5 -14.7 0 0 0
2.5 11.6 -12.6 0 0 0
-14.7 -12.6 42.9 0 0 0
0 0 0 27.6 0 0
0 0 0 0 14.8 0
0 0 0 0 0 20.5
Shear Modulus GV
43 GPa
Bulk Modulus KV
64 GPa
Shear Modulus GR
27 GPa
Bulk Modulus KR
55 GPa
Shear Modulus GVRH
35 GPa
Bulk Modulus KVRH
60 GPa
Elastic Anisotropy
3.16
Poisson's Ratio
0.26

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Hf2NiP (mp-5918) 0.4598 0.000 3
Zr2CoP (mp-29152) 0.4187 0.000 3
Zr2NiP (mp-29153) 0.4435 0.000 3
Hf2CoP (mp-29154) 0.4287 0.000 3
Ba2PtAu (mp-675690) 0.5267 0.003 3
SrCa2In2Ge (mp-619206) 0.4066 0.106 4
CaGa (mp-6914) 0.3233 0.000 2
HfBe (mp-1018057) 0.3680 0.059 2
FeB (mp-1007881) 0.3680 0.006 2
ThAu (mp-1018175) 0.3638 0.000 2
FeB (mp-1080525) 0.3677 0.000 2
Si (mp-1001113) 0.6664 0.490 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Al
Final Energy/Atom
-5.5244 eV
Corrected Energy
-22.0975 eV
Uncorrected energy = -22.0975 eV Corrected energy = -22.0975 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 247101
  • 58209
  • 609650
Submitted by
User remarks:
  • Yttrium aluminium (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)