material

MgZn2

ID:

mp-1124

DOI:

10.17188/1187663


Tags: Magnesium zinc (1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.130 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.003 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.11 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
MgZn2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 46006 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.002 167.2
WS2 (mp-224) <0 0 1> <0 0 1> 0.002 167.2
Al2O3 (mp-1143) <1 0 0> <1 0 1> 0.002 251.8
Mg (mp-153) <0 0 1> <0 0 1> 0.002 167.2
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.003 286.6
C (mp-66) <1 1 1> <0 0 1> 0.006 286.6
BaTiO3 (mp-5986) <1 1 1> <1 0 1> 0.016 201.5
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.017 191.1
LiNbO3 (mp-3731) <1 0 1> <1 0 0> 0.017 310.4
LiNbO3 (mp-3731) <1 0 0> <1 0 0> 0.017 221.7
Mg (mp-153) <1 0 0> <1 0 0> 0.018 133.0
NaCl (mp-22862) <1 1 1> <0 0 1> 0.019 167.2
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.021 143.3
C (mp-66) <1 1 0> <1 0 1> 0.024 251.8
ZrO2 (mp-2858) <1 0 1> <1 0 1> 0.024 302.2
ZnO (mp-2133) <1 1 1> <1 0 1> 0.025 251.8
BN (mp-984) <0 0 1> <0 0 1> 0.026 71.6
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.030 286.6
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.041 286.6
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.046 23.9
SiC (mp-11714) <1 0 1> <1 0 0> 0.046 354.8
PbS (mp-21276) <1 1 0> <1 1 0> 0.047 153.6
Te2W (mp-22693) <0 0 1> <1 0 1> 0.047 201.5
KCl (mp-23193) <1 1 1> <0 0 1> 0.051 71.6
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.052 47.8
KCl (mp-23193) <1 1 0> <1 1 0> 0.056 230.4
GaN (mp-804) <1 1 1> <1 1 1> 0.061 241.3
KTaO3 (mp-3614) <1 1 0> <1 0 1> 0.065 251.8
AlN (mp-661) <1 1 1> <1 0 1> 0.070 201.5
TiO2 (mp-390) <1 0 1> <1 0 1> 0.072 201.5
ZnO (mp-2133) <0 0 1> <0 0 1> 0.073 286.6
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.075 266.1
AlN (mp-661) <0 0 1> <0 0 1> 0.079 214.9
GaN (mp-804) <1 1 0> <1 0 0> 0.082 88.7
Al (mp-134) <1 1 0> <1 0 1> 0.082 251.8
MgO (mp-1265) <1 1 1> <0 0 1> 0.084 95.5
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.085 191.1
C (mp-48) <1 0 0> <1 0 0> 0.087 310.4
LiAlO2 (mp-3427) <1 0 0> <1 0 1> 0.090 100.7
NdGaO3 (mp-3196) <1 0 0> <0 0 1> 0.098 310.5
C (mp-48) <1 1 0> <1 0 0> 0.099 133.0
ZrO2 (mp-2858) <0 1 1> <0 0 1> 0.100 119.4
Te2W (mp-22693) <0 1 1> <1 0 0> 0.101 177.4
CdS (mp-672) <0 0 1> <0 0 1> 0.103 286.6
BN (mp-984) <1 0 0> <1 0 0> 0.104 310.4
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.107 23.9
C (mp-48) <1 1 1> <1 0 0> 0.113 133.0
LiTaO3 (mp-3666) <1 0 1> <1 0 0> 0.113 310.4
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.122 358.2
Ga2O3 (mp-886) <1 0 0> <1 1 1> 0.128 160.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
101 52 36 0 0 0
52 101 36 0 0 0
36 36 123 0 0 0
0 0 0 25 0 0
0 0 0 0 25 0
0 0 0 0 0 24
Compliance Tensor Sij (10-12Pa-1)
14.2 -6.6 -2.2 0 0 0
-6.6 14.2 -2.2 0 0 0
-2.2 -2.2 9.4 0 0 0
0 0 0 40 0 0
0 0 0 0 40 0
0 0 0 0 0 41.5
Shear Modulus GV
28 GPa
Bulk Modulus KV
64 GPa
Shear Modulus GR
27 GPa
Bulk Modulus KR
64 GPa
Shear Modulus GVRH
27 GPa
Bulk Modulus KVRH
64 GPa
Elastic Anisotropy
0.25
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ca2Mg3Si (mp-1095343) 0.1805 0.119 3
Zr2Fe3Ge (mp-21040) 0.0982 0.000 3
Zr2Fe3Si (mp-16336) 0.0501 0.000 3
Mg2Cu3Si (mp-10746) 0.1398 0.000 3
Mn2Co3Ge (mp-22702) 0.1373 0.146 3
TbMg2 (mp-11497) 0.0519 0.015 2
HoMg2 (mp-13499) 0.0517 0.010 2
ScZn2 (mp-13503) 0.0355 0.000 2
CaMg2 (mp-2432) 0.0550 0.000 2
DyMg2 (mp-30602) 0.0436 0.014 2
Co (mp-1072089) 0.2031 0.199 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Zn
Final Energy/Atom
-1.5029 eV
Corrected Energy
-18.0343 eV
-18.0343 eV = -18.0343 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 104897
  • 108587
  • 107545
  • 184412
  • 642928
  • 151382
  • 654727
  • 46006
Submitted by
User remarks:
  • Magnesium zinc (1/2)