Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.230 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.124 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTi3Au |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 345.2 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 258.4 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 164.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 211.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 199.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 149.5 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 201.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 33.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 47.0 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 281.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 83.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 211.4 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 281.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 199.3 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 143.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 211.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 94.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 132.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 47.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 164.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 66.4 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 211.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 16.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 23.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 265.8 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 164.4 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 215.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 16.6 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 28.8 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 215.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 83.0 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 187.9 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 249.1 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 211.4 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 211.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 16.6 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 211.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 199.3 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 258.4 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 201.4 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 115.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 249.1 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 86.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 299.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 83.0 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 201.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 149.5 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 201.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 33.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 47.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
122 | 74 | 74 | 0 | 0 | 0 |
74 | 122 | 74 | 0 | 0 | 0 |
74 | 74 | 122 | 0 | 0 | 0 |
0 | 0 | 0 | 6 | 0 | 0 |
0 | 0 | 0 | 0 | 6 | 0 |
0 | 0 | 0 | 0 | 0 | 6 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
15.2 | -5.8 | -5.8 | 0 | 0 | 0 |
-5.8 | 15.2 | -5.8 | 0 | 0 | 0 |
-5.8 | -5.8 | 15.2 | 0 | 0 | 0 |
0 | 0 | 0 | 157.8 | 0 | 0 |
0 | 0 | 0 | 0 | 157.8 | 0 |
0 | 0 | 0 | 0 | 0 | 157.8 |
Shear Modulus GV13 GPa |
Bulk Modulus KV90 GPa |
Shear Modulus GR9 GPa |
Bulk Modulus KR90 GPa |
Shear Modulus GVRH11 GPa |
Bulk Modulus KVRH90 GPa |
Elastic Anisotropy2.43 |
Poisson's Ratio0.44 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.000 | 3 |
LiCa6Ge (mp-12609) | 0.0000 | 0.180 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.066 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
Fe3Ge (mp-20344) | 0.0000 | 0.004 | 2 |
V3Au (mp-570698) | 0.0000 | 0.101 | 2 |
Ce3Ga (mp-19920) | 0.0000 | 0.000 | 2 |
VC3 (mp-1067129) | 0.0000 | 2.503 | 2 |
ErIn3 (mp-1291) | 0.0000 | 0.000 | 2 |
H2 (mp-634659) | 0.0000 | 0.000 | 1 |
Sn (mp-1022725) | 0.0000 | 0.037 | 1 |
Sr (mp-76) | 0.0000 | 0.006 | 1 |
Ni (mp-1056486) | 0.0000 | 0.000 | 1 |
Cd (mp-1096861) | 0.0000 | 0.001 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv Au |
Final Energy/Atom-6.9698 eV |
Corrected Energy-27.8792 eV
-27.8792 eV = -27.8792 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)