material

Ta2Be

ID:

mp-11278

DOI:

10.17188/1187700


Tags: Beryllium tantalum (1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.160 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
13.76 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mcm [140]
Hall
-I 4 2c
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 58738 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
NaCl (mp-22862) <1 0 0> <0 0 1> 0.002 291.9
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.003 146.0
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.005 73.0
GaN (mp-804) <0 0 1> <1 1 0> 0.021 125.7
CdWO4 (mp-19387) <1 0 0> <1 0 1> 0.034 94.0
Al (mp-134) <1 0 0> <0 0 1> 0.034 146.0
ZnO (mp-2133) <1 0 1> <1 0 0> 0.041 59.3
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.044 88.9
ZnO (mp-2133) <0 0 1> <1 1 0> 0.050 83.8
MgO (mp-1265) <1 0 0> <0 0 1> 0.050 36.5
C (mp-48) <0 0 1> <1 1 0> 0.055 41.9
TiO2 (mp-390) <0 0 1> <0 0 1> 0.057 73.0
KTaO3 (mp-3614) <1 1 1> <1 1 0> 0.067 83.8
PbS (mp-21276) <1 1 1> <1 1 0> 0.069 125.7
NdGaO3 (mp-3196) <0 1 0> <1 0 0> 0.088 296.4
Si (mp-149) <1 1 0> <1 0 0> 0.089 296.4
CeO2 (mp-20194) <1 1 0> <1 0 0> 0.090 296.4
CdS (mp-672) <1 0 1> <1 0 0> 0.111 296.4
CdWO4 (mp-19387) <0 1 1> <1 0 0> 0.112 326.0
Te2W (mp-22693) <1 0 0> <1 0 0> 0.139 296.4
Al (mp-134) <1 1 0> <1 0 0> 0.139 326.0
Al (mp-134) <1 1 1> <1 1 0> 0.145 83.8
ZnO (mp-2133) <1 0 0> <1 0 0> 0.146 207.5
PbS (mp-21276) <1 0 0> <0 0 1> 0.155 36.5
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.157 146.0
BN (mp-984) <1 1 0> <1 0 1> 0.165 235.1
MgO (mp-1265) <1 1 0> <1 0 0> 0.194 177.8
LiGaO2 (mp-5854) <1 1 0> <1 1 0> 0.206 293.4
NdGaO3 (mp-3196) <0 0 1> <1 1 1> 0.214 333.4
LiF (mp-1138) <1 1 0> <1 0 0> 0.221 326.0
KTaO3 (mp-3614) <1 1 0> <1 0 0> 0.230 326.0
LiGaO2 (mp-5854) <0 1 1> <0 0 1> 0.259 219.0
GaP (mp-2490) <1 1 0> <1 0 0> 0.262 296.4
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.275 291.9
PbS (mp-21276) <1 1 0> <1 0 0> 0.320 207.5
Ni (mp-23) <1 1 1> <1 1 0> 0.322 41.9
WS2 (mp-224) <1 1 1> <1 0 1> 0.336 235.1
AlN (mp-661) <1 0 1> <1 0 0> 0.337 326.0
MgO (mp-1265) <1 1 1> <0 0 1> 0.343 255.4
Cu (mp-30) <1 0 0> <1 1 0> 0.354 251.5
TeO2 (mp-2125) <1 1 0> <0 0 1> 0.370 291.9
CaF2 (mp-2741) <1 1 0> <1 0 0> 0.371 296.4
WS2 (mp-224) <0 0 1> <1 1 0> 0.374 125.7
GaAs (mp-2534) <1 0 0> <0 0 1> 0.375 291.9
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.376 125.7
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.403 209.6
CdS (mp-672) <1 0 0> <1 1 0> 0.450 293.4
MgF2 (mp-1249) <1 0 0> <1 1 1> 0.454 222.3
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.458 291.9
SiC (mp-11714) <1 1 0> <1 0 0> 0.464 266.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
322 124 124 0 0 0
124 314 118 0 0 0
124 118 314 0 0 0
0 0 0 128 0 0
0 0 0 0 134 0
0 0 0 0 0 134
Compliance Tensor Sij (10-12Pa-1)
4 -1.2 -1.2 0 0 0
-1.2 4 -1.1 0 0 0
-1.2 -1.1 4 0 0 0
0 0 0 7.8 0 0
0 0 0 0 7.5 0
0 0 0 0 0 7.5
Shear Modulus GV
118 GPa
Bulk Modulus KV
187 GPa
Shear Modulus GR
115 GPa
Bulk Modulus KR
187 GPa
Shear Modulus GVRH
117 GPa
Bulk Modulus KVRH
187 GPa
Elastic Anisotropy
0.12
Poisson's Ratio
0.24

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nb4CoP (mp-21447) 0.1320 0.053 3
Nb4SiNi (mp-22396) 0.1825 0.004 3
Ta4FeP (mp-22444) 0.2488 0.055 3
Nb4CoSi (mp-10003) 0.2735 0.013 3
Zr4CuP (mp-581733) 0.1987 0.063 3
Tl2Pt (mp-571160) 0.0368 0.007 2
Th2Pd (mp-1148) 0.0340 0.000 2
Ta2Co (mp-574) 0.0051 0.000 2
FeSn2 (mp-22752) 0.0384 0.014 2
FeSn2 (mp-1077439) 0.0464 0.014 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ta_pv Be_sv
Final Energy/Atom
-9.3119 eV
Corrected Energy
-55.8717 eV
Uncorrected energy = -55.8717 eV Corrected energy = -55.8717 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 58738
Submitted by
User remarks:
  • Beryllium tantalum (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)