material

Be2W

ID:

mp-11282

DOI:

10.17188/1187705


Tags: Tungsten beryllide (1/2) Beryllium tungsten (2/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.304 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.61 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 58754 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Au (mp-81) <1 1 1> <0 0 1> 0.000 120.5
TePb (mp-19717) <1 1 1> <0 0 1> 0.001 223.8
MoS2 (mp-1434) <0 0 1> <1 0 1> 0.005 184.8
WS2 (mp-224) <0 0 1> <1 0 1> 0.005 184.8
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.006 51.6
NaCl (mp-22862) <1 1 1> <0 0 1> 0.008 223.8
Mg (mp-153) <0 0 1> <1 0 1> 0.008 184.8
Si (mp-149) <1 1 1> <0 0 1> 0.008 51.6
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.014 17.2
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.015 68.9
C (mp-48) <0 0 1> <0 0 1> 0.020 68.9
Ag (mp-124) <1 1 1> <0 0 1> 0.020 120.5
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.030 327.1
Ga2O3 (mp-886) <1 1 0> <1 0 0> 0.032 294.4
Si (mp-149) <1 0 0> <0 0 1> 0.035 327.1
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.044 68.9
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.047 226.6
CdS (mp-672) <1 0 1> <1 1 0> 0.049 226.6
Si (mp-149) <1 1 0> <1 1 0> 0.050 170.0
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.054 170.0
MgO (mp-1265) <1 0 0> <1 1 1> 0.056 236.8
SiC (mp-7631) <1 0 1> <1 1 1> 0.057 236.8
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.069 206.6
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.094 258.2
Bi2Te3 (mp-34202) <1 0 0> <0 0 1> 0.102 137.7
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.102 163.5
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.105 163.5
MoSe2 (mp-1634) <1 0 1> <1 0 1> 0.110 258.7
GaP (mp-2490) <1 1 0> <1 1 0> 0.110 170.0
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.121 196.3
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.139 327.1
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.146 258.2
LiAlO2 (mp-3427) <1 0 1> <1 0 1> 0.146 258.7
Fe2O3 (mp-24972) <1 0 1> <1 1 0> 0.147 226.6
Cu (mp-30) <1 1 1> <0 0 1> 0.153 68.9
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.163 170.0
SiC (mp-11714) <1 0 0> <1 0 1> 0.166 221.8
TiO2 (mp-2657) <1 1 1> <1 0 1> 0.180 147.8
LiGaO2 (mp-5854) <0 1 0> <1 0 1> 0.180 332.7
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.182 170.0
LiTaO3 (mp-3666) <1 0 1> <1 1 0> 0.194 226.6
BN (mp-984) <1 1 1> <1 1 1> 0.201 236.8
LaF3 (mp-905) <1 0 1> <1 1 0> 0.205 283.3
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.222 223.8
PbSe (mp-2201) <1 0 0> <1 0 0> 0.222 196.3
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.239 163.5
GaN (mp-804) <1 0 0> <1 0 1> 0.243 332.7
SiC (mp-11714) <0 0 1> <0 0 1> 0.249 154.9
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.252 294.4
GaP (mp-2490) <1 1 1> <0 0 1> 0.255 51.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
449 96 108 0 0 0
96 449 108 0 0 0
108 108 440 0 0 0
0 0 0 165 0 0
0 0 0 0 165 0
0 0 0 0 0 177
Compliance Tensor Sij (10-12Pa-1)
2.4 -0.4 -0.5 0 0 0
-0.4 2.4 -0.5 0 0 0
-0.5 -0.5 2.5 0 0 0
0 0 0 6.1 0 0
0 0 0 0 6.1 0
0 0 0 0 0 5.7
Shear Modulus GV
170 GPa
Bulk Modulus KV
218 GPa
Shear Modulus GR
170 GPa
Bulk Modulus KR
218 GPa
Shear Modulus GVRH
170 GPa
Bulk Modulus KVRH
218 GPa
Elastic Anisotropy
0.01
Poisson's Ratio
0.19

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NdMgNi4 (mp-11194) 0.1428 0.000 3
YbNi4Au (mp-1024977) 0.1432 0.040 3
Zr2Fe3Ge (mp-21040) 0.1212 0.000 3
Zr2Fe3Si (mp-16336) 0.1251 0.000 3
GdInCu4 (mp-1077293) 0.1433 0.000 3
ErMn2 (mp-1095451) 0.0359 0.042 2
Be2Cr (mp-30438) 0.0251 0.000 2
ScMn2 (mp-2039) 0.0305 0.000 2
Be2Mo (mp-1677) 0.0294 0.000 2
Zn2Ag (mp-1093999) 0.0388 0.014 2
Co (mp-1072089) 0.1432 0.199 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Be_sv W_pv
Final Energy/Atom
-7.1159 eV
Corrected Energy
-85.3909 eV
Uncorrected energy = -85.3909 eV Corrected energy = -85.3909 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 58754
  • 616501
Submitted by
User remarks:
  • Beryllium tungsten (2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)