Material Details

Final Magnetic Moment
0.025 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.152 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.33 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 58961 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CsI (mp-614603) <1 1 0> <1 1 0> 0.002 174.4
BN (mp-984) <0 0 1> <1 1 1> 0.003 71.2
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.004 164.4
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.011 284.8
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.016 71.2
KCl (mp-23193) <1 0 0> <1 0 0> 0.017 41.1
GaAs (mp-2534) <1 0 0> <1 0 0> 0.018 164.4
KCl (mp-23193) <1 1 0> <1 1 0> 0.019 58.1
KCl (mp-23193) <1 1 1> <1 1 1> 0.019 71.2
GaN (mp-804) <0 0 1> <1 0 0> 0.025 287.8
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.026 246.7
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.030 164.4
ZnO (mp-2133) <0 0 1> <1 0 0> 0.037 328.9
Al (mp-134) <1 0 0> <1 0 0> 0.041 82.2
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.044 116.3
MgO (mp-1265) <1 0 0> <1 0 0> 0.046 164.4
SiC (mp-8062) <1 0 0> <1 0 0> 0.047 328.9
MgO (mp-1265) <1 1 0> <1 1 0> 0.050 232.6
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.058 284.8
Ge (mp-32) <1 0 0> <1 0 0> 0.061 164.4
C (mp-66) <1 0 0> <1 0 0> 0.066 164.4
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.069 174.4
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.072 328.9
C (mp-66) <1 1 1> <1 1 1> 0.073 284.8
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.075 232.6
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.076 71.2
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.092 82.2
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.096 174.4
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.105 284.8
Au (mp-81) <1 1 1> <1 1 1> 0.111 213.6
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.122 174.4
PbS (mp-21276) <1 0 0> <1 0 0> 0.123 328.9
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.125 213.6
LiF (mp-1138) <1 0 0> <1 0 0> 0.125 82.2
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.135 174.4
Mg (mp-153) <0 0 1> <1 1 0> 0.136 174.4
NaCl (mp-22862) <1 0 0> <1 0 0> 0.145 164.4
CdS (mp-672) <0 0 1> <1 1 0> 0.150 232.6
Ni (mp-23) <1 1 0> <1 0 0> 0.155 328.9
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.179 205.6
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.191 142.4
GaP (mp-2490) <1 1 0> <1 1 0> 0.194 174.4
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.194 164.4
GaP (mp-2490) <1 1 1> <1 1 1> 0.199 213.6
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.201 174.4
WS2 (mp-224) <0 0 1> <1 1 0> 0.202 174.4
Ni (mp-23) <1 0 0> <1 0 0> 0.202 205.6
Cu (mp-30) <1 0 0> <1 0 0> 0.207 205.6
Ag (mp-124) <1 1 1> <1 1 1> 0.221 213.6
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.235 290.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
155 95 95 0 0 0
95 155 95 0 0 0
95 95 155 0 0 0
0 0 0 73 0 0
0 0 0 0 73 0
0 0 0 0 0 73
Compliance Tensor Sij (10-12Pa-1)
12.2 -4.6 -4.6 0 0 0
-4.6 12.2 -4.6 0 0 0
-4.6 -4.6 12.2 0 0 0
0 0 0 13.7 0 0
0 0 0 0 13.7 0
0 0 0 0 0 13.7
Shear Modulus GV
56 GPa
Bulk Modulus KV
115 GPa
Shear Modulus GR
46 GPa
Bulk Modulus KR
115 GPa
Shear Modulus GVRH
51 GPa
Bulk Modulus KVRH
115 GPa
Elastic Anisotropy
1.05
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
SmInCu2 (mp-21475) 0.0000 0.016 3
MnNi2Sn (mp-20440) 0.0000 0.010 3
CuSnRh2 (mp-30595) 0.0000 0.000 3
TiCuHg2 (mp-11882) 0.0000 0.253 3
LiAl2Pt (mp-30819) 0.0000 0.000 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSnAu (mp-7554) 0.0000 0.088 4
VFeCoGe (mp-1063914) 0.0000 0.000 4
LiMgSbPd (mp-10179) 0.0000 0.096 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
NaIn (mp-20628) 0.0000 0.000 2
AlCu3 (mp-12777) 0.0000 0.025 2
LiZn (mp-1934) 0.0000 0.000 2
LaF3 (mp-13181) 0.0000 0.181 2
CeCd3 (mp-2863) 0.0000 0.000 2
Mg (mp-110) 0.0000 0.022 1
He (mp-23158) 0.0000 0.000 1
Mo (mp-129) 0.0000 0.000 1
Pu (mp-107) 0.0000 0.546 1
Tb (mp-11446) 0.0000 0.148 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Cd Cu_pv
Final Energy/Atom
-4.5648 eV
Corrected Energy
-18.2593 eV
Uncorrected energy = -18.2593 eV Corrected energy = -18.2593 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 58961
Submitted by
User remarks:
  • Cadmium copper zirconium (1/2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)