material

Cd2Hg

ID:

mp-11299

DOI:

10.17188/1187720


Tags: Cadmium mercury (2/1) - LT Cadmium mercury (2/1)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.015 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.015 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.77 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Cd + Hg
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 58983 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Cu (mp-30) <1 0 0> <0 0 1> 0.000 65.4
KCl (mp-23193) <1 0 0> <0 0 1> 0.000 81.8
TiO2 (mp-390) <1 1 0> <1 0 1> 0.001 157.3
Ge(Bi3O5)4 (mp-23352) <1 0 0> <0 0 1> 0.001 212.6
Al (mp-134) <1 0 0> <0 0 1> 0.001 16.4
TiO2 (mp-390) <0 0 1> <0 0 1> 0.003 130.8
AlN (mp-661) <1 0 1> <0 0 1> 0.003 196.2
ZnO (mp-2133) <1 1 0> <1 1 0> 0.005 151.7
KTaO3 (mp-3614) <1 1 0> <0 0 1> 0.008 114.5
NaCl (mp-22862) <1 1 0> <0 0 1> 0.009 228.9
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.011 16.4
GaSe (mp-1943) <1 0 0> <1 1 0> 0.012 202.3
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.012 310.7
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.012 245.3
Ni (mp-23) <1 1 0> <0 0 1> 0.016 245.3
Ge (mp-32) <1 1 1> <1 0 0> 0.016 286.1
GaAs (mp-2534) <1 1 1> <1 0 0> 0.016 286.1
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.019 32.7
Al (mp-134) <1 1 0> <0 0 1> 0.021 114.5
ZnO (mp-2133) <1 1 1> <1 1 1> 0.022 159.5
ZnSe (mp-1190) <1 1 1> <1 0 0> 0.023 286.1
NaCl (mp-22862) <1 0 0> <0 0 1> 0.024 32.7
Fe2O3 (mp-24972) <1 1 1> <1 0 0> 0.024 250.4
DyScO3 (mp-31120) <0 1 0> <0 0 1> 0.024 130.8
TeO2 (mp-2125) <1 1 0> <0 0 1> 0.025 98.1
GaN (mp-804) <1 0 1> <1 0 0> 0.026 286.1
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.029 147.2
BN (mp-984) <1 1 1> <1 0 1> 0.030 236.0
CdS (mp-672) <1 0 0> <0 0 1> 0.031 261.6
GaAs (mp-2534) <1 0 0> <0 0 1> 0.034 32.7
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.034 130.8
MoSe2 (mp-1634) <1 1 1> <1 1 1> 0.038 265.8
Mg (mp-153) <0 0 1> <0 0 1> 0.038 327.0
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.043 252.9
TeO2 (mp-2125) <1 0 0> <1 1 1> 0.046 212.6
CdWO4 (mp-19387) <1 0 1> <1 0 1> 0.046 314.6
MoSe2 (mp-1634) <1 0 0> <0 0 1> 0.046 310.7
LaF3 (mp-905) <1 0 0> <0 0 1> 0.048 212.6
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.048 327.0
LiGaO2 (mp-5854) <1 0 0> <1 0 1> 0.049 314.6
Te2W (mp-22693) <0 0 1> <0 0 1> 0.049 245.3
Cu (mp-30) <1 1 1> <1 0 0> 0.054 178.8
GaSe (mp-1943) <0 0 1> <0 0 1> 0.056 261.6
MgO (mp-1265) <1 0 0> <0 0 1> 0.061 147.2
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.064 252.9
ZrO2 (mp-2858) <1 1 -1> <1 0 0> 0.065 321.9
Ge (mp-32) <1 0 0> <0 0 1> 0.066 32.7
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.067 147.2
AlN (mp-661) <0 0 1> <0 0 1> 0.067 228.9
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.070 118.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
42 30 27 0 0 0
30 42 27 0 0 0
27 27 102 0 0 0
0 0 0 15 0 0
0 0 0 0 15 0
0 0 0 0 0 11
Compliance Tensor Sij (10-12Pa-1)
53.3 -35.9 -4.7 0 0 0
-35.9 53.3 -4.7 0 0 0
-4.7 -4.7 12.4 0 0 0
0 0 0 66 0 0
0 0 0 0 66 0
0 0 0 0 0 90.9
Shear Modulus GV
15 GPa
Bulk Modulus KV
40 GPa
Shear Modulus GR
11 GPa
Bulk Modulus KR
35 GPa
Shear Modulus GVRH
13 GPa
Bulk Modulus KVRH
37 GPa
Elastic Anisotropy
1.71
Poisson's Ratio
0.34

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LaSb2Au (mp-675224) 0.4342 0.263 3
HoAu2 (mp-990) 0.4416 0.000 2
ZrSi (mp-1066771) 0.2946 0.884 2
GdAu2 (mp-1063174) 0.4412 0.000 2
MgHg2 (mp-11464) 0.2813 0.022 2
CdHg2 (mp-30488) 0.0032 0.031 2
Si (mp-1056579) 0.3152 0.486 1
Sc (mp-601273) 0.3824 0.128 1
Pa (mp-62) 0.4475 0.027 1
Cu (mp-1059259) 0.5460 0.143 1
Sn (mp-55) 0.5551 0.063 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cd Hg
Final Energy/Atom
-0.7014 eV
Corrected Energy
-2.1043 eV
Uncorrected energy = -2.1043 eV Corrected energy = -2.1043 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 58983
  • 619972
Submitted by
User remarks:
  • Cadmium mercury (2/1) - LT

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)