material

Tc

ID:

mp-113

DOI:

10.17188/1187721


Tags: Technetium

Material Details

Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.000 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
11.15 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 52498 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgO (mp-1265) <1 1 1> <0 0 1> 0.001 125.4
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.005 26.4
WS2 (mp-224) <0 0 1> <0 0 1> 0.006 26.4
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.010 204.6
Mg (mp-153) <0 0 1> <0 0 1> 0.010 26.4
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.013 125.4
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.019 165.0
WS2 (mp-224) <1 1 1> <0 0 1> 0.026 79.2
Mg (mp-153) <1 1 1> <0 0 1> 0.027 211.2
CdS (mp-672) <0 0 1> <0 0 1> 0.041 46.2
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.048 85.8
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.049 85.8
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 0.053 125.4
Ni (mp-23) <1 1 1> <0 0 1> 0.066 85.8
LiNbO3 (mp-3731) <1 0 1> <1 1 1> 0.068 155.0
C (mp-66) <1 0 0> <1 0 1> 0.070 152.6
PbSe (mp-2201) <1 0 0> <1 0 0> 0.088 195.3
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.098 231.9
YAlO3 (mp-3792) <0 1 0> <1 1 1> 0.102 155.0
GaP (mp-2490) <1 0 0> <0 0 1> 0.106 211.2
AlN (mp-661) <1 0 0> <1 0 1> 0.107 124.9
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.110 132.0
YVO4 (mp-19133) <1 0 1> <0 0 1> 0.112 138.6
LiAlO2 (mp-3427) <1 0 1> <1 0 0> 0.134 85.4
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.137 132.0
Fe2O3 (mp-24972) <1 1 0> <1 0 0> 0.141 122.1
SiO2 (mp-6930) <1 1 1> <1 0 0> 0.145 158.7
SiO2 (mp-6930) <1 0 0> <1 0 0> 0.146 195.3
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.150 52.8
LiF (mp-1138) <1 1 1> <0 0 1> 0.156 85.8
GaSb (mp-1156) <1 0 0> <1 0 0> 0.156 195.3
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.157 19.8
Ga2O3 (mp-886) <1 1 0> <1 0 1> 0.177 291.4
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.183 195.3
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.184 211.2
Si (mp-149) <1 0 0> <0 0 1> 0.191 211.2
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.205 211.2
WS2 (mp-224) <1 1 0> <0 0 1> 0.206 79.2
Al2O3 (mp-1143) <1 0 1> <1 1 1> 0.209 66.4
CdSe (mp-2691) <1 0 0> <1 0 0> 0.225 195.3
Te2Mo (mp-602) <1 0 0> <0 0 1> 0.227 217.8
WSe2 (mp-1821) <1 0 1> <1 0 1> 0.240 152.6
Al (mp-134) <1 1 1> <0 0 1> 0.241 85.8
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.242 46.2
KP(HO2)2 (mp-23959) <0 1 1> <0 0 1> 0.247 217.8
MoSe2 (mp-1634) <1 1 1> <1 0 1> 0.254 180.4
Fe2O3 (mp-24972) <1 0 0> <0 0 1> 0.260 211.2
ZrO2 (mp-2858) <1 0 1> <1 0 0> 0.274 85.4
LaF3 (mp-905) <1 1 0> <0 0 1> 0.275 92.4
CsI (mp-614603) <1 1 1> <0 0 1> 0.278 105.6
Up to 50 entries displayed.
minimal coincident interface area.

Surfaces

Reference for surface energies and properties: Periodic Table of Wulff Shapes
Weighted surface energy γ
2.61 J/m2 (0.16 eV/Å2)
Weighted work function Φ
4.31 eV
Shape factor η
5.09
Surface energy anisotropy αγ
0.087
Miller Indices
(hklm)
Surface Energy
(J/m2, eV/Å2)
Work Function
(eV)
Area Fraction Slab
(CIF)
(0001) 2.25, 0.14 4.63 0.21
(1010) 2.53, 0.16 4.22 0.28
(1120) 2.69, 0.17 4.01 0.09
(2130) 2.72, 0.17 4.05 0.00
(2021) 2.75, 0.17 4.57 0.09
(2241) 2.82, 0.18 3.94 0.00
(1012) 2.83, 0.18 4.35 0.19
(1121) 2.84, 0.18 3.80 0.07
(2131) 2.85, 0.18 3.91 0.00
(2112) 2.91, 0.18 4.19 0.08
(2132) 2.95, 0.18 4.21 0.00
(1011) 3.28, 0.20 3.76 0.00

Grain Boundaries

Reference for grain boundary energies and properties:
Sigma, Σ
type
rotation axis rotation angle GB plane Energy, 𝛾GB
(J/m2)
Work of Separation, Wsep
(J/m2)
Structure
(CIF)
7 twist [0001] 21.79 (0001) 0.67 3.80

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
497 222 174 0 0 0
222 497 174 0 0 0
174 174 566 0 0 0
0 0 0 126 0 0
0 0 0 0 126 0
0 0 0 0 0 137
Compliance Tensor Sij (10-12Pa-1)
2.6 -1 -0.5 0 0 0
-1 2.6 -0.5 0 0 0
-0.5 -0.5 2.1 0 0 0
0 0 0 7.9 0 0
0 0 0 0 7.9 0
0 0 0 0 0 7.3
Shear Modulus GV
144 GPa
Bulk Modulus KV
300 GPa
Shear Modulus GR
140 GPa
Bulk Modulus KR
300 GPa
Shear Modulus GVRH
142 GPa
Bulk Modulus KVRH
300 GPa
Elastic Anisotropy
0.13
Poisson's Ratio
0.30

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -10.360 14.605 16.515 6.579
pack_evans_james -10.360 14.606 1.829 3.529
vinet -10.362 14.595 16.827 5.406
tait -10.361 14.595 1.850 5.674
birch_euler -10.360 14.603 2.071 0.542
pourier_tarantola -10.365 14.591 0.319 2.589
birch_lagrange -10.380 14.600 1.191 6.205
murnaghan -10.357 14.621 1.784 3.390
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Cr8Ni50Mo15W2 (mp-767372) 0.2663 0.028 4
CrFeCoNi (mp-1012640) 0.1815 0.065 4
CrFeCoNi (mp-1096923) 0.4007 0.193 4
HfZr (mp-983459) 0.0133 0.002 2
CaAc3 (mp-983567) 0.0113 0.059 2
TbZr (mp-978918) 0.0104 0.119 2
Ir3W (mp-30745) 0.0125 0.000 2
CoTc3 (mp-865733) 0.0155 0.000 2
Xe (mp-570510) 0.0150 0.000 1
Gd (mp-155) 0.0119 0.000 1
Li (mp-10173) 0.0044 0.003 1
Gd (mp-910209) 0.0134 0.000 1
Zr (mp-131) 0.0119 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Tc_pv
Final Energy/Atom
-10.3606 eV
Corrected Energy
-20.7212 eV
-20.7212 eV = -20.7212 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 426979
  • 653014
  • 653011
  • 52498
  • 653012
  • 76953
  • 182009
Submitted by
User remarks:
  • Technetium

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)