material

MgCuSn

ID:

mp-11361

DOI:

10.17188/1187763


Tags: Copper magnesium tin (1/1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.154 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.66 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
F43m [216]
Hall
F 4 2 3
Point Group
43m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 628345 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiF (mp-1138) <1 1 1> <1 1 1> 0.000 202.1
GaSe (mp-1943) <0 0 1> <1 1 1> 0.000 202.1
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.001 220.0
Ag (mp-124) <1 0 0> <1 0 0> 0.001 155.6
Ag (mp-124) <1 1 0> <1 1 0> 0.001 220.0
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.001 194.5
Ni (mp-23) <1 1 0> <1 1 0> 0.002 330.1
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.003 311.2
PbSe (mp-2201) <1 0 0> <1 0 0> 0.005 38.9
PbSe (mp-2201) <1 1 0> <1 1 0> 0.005 55.0
PbSe (mp-2201) <1 1 1> <1 1 1> 0.005 67.4
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.007 155.6
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.007 67.4
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.008 67.4
CdTe (mp-406) <1 0 0> <1 0 0> 0.008 350.1
InSb (mp-20012) <1 0 0> <1 0 0> 0.013 350.1
GaSb (mp-1156) <1 0 0> <1 0 0> 0.014 38.9
GaSb (mp-1156) <1 1 0> <1 1 0> 0.015 55.0
GaSb (mp-1156) <1 1 1> <1 1 1> 0.015 67.4
Au (mp-81) <1 0 0> <1 0 0> 0.019 155.6
Au (mp-81) <1 1 0> <1 1 0> 0.019 220.0
Au (mp-81) <1 1 1> <1 1 1> 0.020 269.5
Cu (mp-30) <1 0 0> <1 1 0> 0.022 275.0
AlN (mp-661) <0 0 1> <1 0 0> 0.023 272.3
CsI (mp-614603) <1 0 0> <1 0 0> 0.026 311.2
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.026 116.7
CdSe (mp-2691) <1 0 0> <1 0 0> 0.026 38.9
CdSe (mp-2691) <1 1 0> <1 1 0> 0.027 55.0
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.028 165.0
CdSe (mp-2691) <1 1 1> <1 1 1> 0.028 67.4
Cu (mp-30) <1 1 0> <1 1 0> 0.035 55.0
Cu (mp-30) <1 1 1> <1 1 1> 0.035 67.4
TiO2 (mp-2657) <1 1 1> <1 1 1> 0.044 202.1
Mg (mp-153) <0 0 1> <1 1 1> 0.045 269.5
GaN (mp-804) <0 0 1> <1 0 0> 0.047 311.2
MgO (mp-1265) <1 0 0> <1 0 0> 0.047 311.2
WS2 (mp-224) <0 0 1> <1 0 0> 0.051 311.2
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.052 311.2
Ga2O3 (mp-886) <1 0 0> <1 1 1> 0.052 269.5
ZnO (mp-2133) <1 1 0> <1 1 0> 0.055 330.1
ZnO (mp-2133) <1 0 1> <1 1 0> 0.055 275.0
Te2W (mp-22693) <0 1 0> <1 1 1> 0.070 269.5
ZnO (mp-2133) <1 1 1> <1 1 0> 0.078 220.0
SiC (mp-8062) <1 0 0> <1 0 0> 0.085 38.9
SiC (mp-11714) <0 0 1> <1 1 0> 0.086 165.0
SiC (mp-7631) <1 1 0> <1 1 0> 0.086 165.0
Te2Mo (mp-602) <1 0 0> <1 1 1> 0.086 269.5
Y3Fe5O12 (mp-19648) <1 0 0> <1 0 0> 0.087 155.6
SiC (mp-8062) <1 1 0> <1 1 0> 0.089 55.0
SiC (mp-7631) <0 0 1> <1 1 0> 0.089 165.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
95 47 47 0 0 0
47 95 47 0 0 0
47 47 95 0 0 0
0 0 0 34 0 0
0 0 0 0 34 0
0 0 0 0 0 34
Compliance Tensor Sij (10-12Pa-1)
15.5 -5.1 -5.1 0 0 0
-5.1 15.5 -5.1 0 0 0
-5.1 -5.1 15.5 0 0 0
0 0 0 29.2 0 0
0 0 0 0 29.2 0
0 0 0 0 0 29.2
Shear Modulus GV
30 GPa
Bulk Modulus KV
63 GPa
Shear Modulus GR
29 GPa
Bulk Modulus KR
63 GPa
Shear Modulus GVRH
30 GPa
Bulk Modulus KVRH
63 GPa
Elastic Anisotropy
0.14
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
MgCuBi (mp-30449) 0.0000 0.041 3
YNiBi (mp-30460) 0.0000 0.000 3
HfSbRu (mp-31456) 0.0000 0.030 3
VCoSb (mp-4076) 0.0000 0.006 3
MgSnAu (mp-5549) 0.0000 0.000 3
AcH2 (mp-24147) 0.0000 0.000 2
DyH2 (mp-24151) 0.0000 0.000 2
PbF2 (mp-315) 0.0000 0.000 2
K2Te (mp-1747) 0.0000 0.000 2
Pu2Mg (mp-21152) 0.0000 0.720 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Cu_pv Sn_d
Final Energy/Atom
-3.3831 eV
Corrected Energy
-10.1493 eV
Uncorrected energy = -10.1493 eV Corrected energy = -10.1493 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 628345
Submitted by
User remarks:
  • Copper magnesium tin (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)